Dow Engage® 8200 Polyolefin Elastomer

Category Polymer , Thermoplastic , Elastomer, TPE , Thermoplastic Elastomer, Melt-Processible Rubber
Manufacturer Dow Chemical
Trade Name Engage®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dow Engage® 8200 Polyolefin Elastomer.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Description: Engage® 8200 and Engage® 8207 polyolefin elastomers are ethylene-octene copolymers that have excellent flow characteristics and performs well in a wide range of general purpose thermoplastic elastomer applications. They provide good impact properties in blends with polypropylene (PP) and polyethylene (PE), especially in applications requiring slightly higher melt flow. Engage® 8200 and Engage® 8207 also provide high filler loading capability. They have excellent electrical properties, and when cross-linked give exceptional heat aging, compression set, and weather resistance properties. Engage® 8207 is Engage® 8200 with a nominal loose talc coating. The talc is untreated, with a 1 micron particle size. The product form is free-flowing pellets.Information provided by manufacturer.This former DuPont Dow Elastomers product line is now produced by Dow Chemical.
Physical Properties Metric English Comments
Density 0.870 g/cc
0.0314 lb/in³
ASTM D792
Mooney Viscosity 8.0

@Temperature 121 °C
8.0

@Temperature 250 °F
ML 1 + 4; ASTM D1646
Melt Index of Compound 5.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
5.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore A 75
75
ASTM D2240
Hardness, Shore D 21
21
ASTM D2240
Tensile Strength, Ultimate 6.90 MPa
1000 psi
508 mm/min; ASTM D638
Tensile Strength, Yield 2.10 MPa
305 psi
508 mm/min; ASTM D638
Elongation at Break 1030 %
1030 %
508 mm/min; ASTM D638
2% Secant Modulus 0.0121 GPa
1.75 ksi
ASTM D790
Thermal Properties Metric English Comments
Melting Point 60.0 °C
140 °F
DSC, 10°C/min; DuPont Test
Brittleness Temperature <= -76.0 °C
<= -105 °F
ASTM D746
Descriptive Properties Value Comments
Comonomer Content 38 wt%
Dow Method (<sup>13</sup>C NMR/FTIR)
Users viewing this material also viewed the following: