| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.05 g/cc | 0.0379 lb/in³ | |
| Water Absorption | 0.10 % | 0.10 % | |
| Moisture Absorption at Equilibrium | 0.10 % | 0.10 % | |
| Linear Mold Shrinkage, Flow | 0.0055 cm/cm | 0.0055 in/in | |
| Melt Flow | 5.5 g/10 min <br>@Load 5.00 kg,<br> Temperature 200 °C |
5.5 g/10 min <br>@Load 11.0 lb,<br> Temperature 392 °F |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength, Yield | 31.0 MPa | 4500 psi | |
| Elongation at Break | 30 % | 30 % | |
| Elongation at Yield | 1.6 % | 1.6 % | |
| Tensile Modulus | 2.05 GPa | 297 ksi | |
| Charpy Impact Unnotched | 12.0 J/cm² | 57.1 ft-lb/in² | |
| 7.00 J/cm² <br>@Temperature -30.0 °C |
33.3 ft-lb/in² <br>@Temperature -22.0 °F |
||
| Charpy Impact, Notched | 1.30 J/cm² | 6.19 ft-lb/in² |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear, Parallel to Flow | 100 µm/m-°C <br>@Temperature 20.0 °C |
55.6 µin/in-°F <br>@Temperature 68.0 °F |
|
| Deflection Temperature at 0.46 MPa (66 psi) | 88.0 °C | 190 °F | |
| Deflection Temperature at 1.8 MPa (264 psi) | 78.0 °C | 172 °F | |
| Vicat Softening Point | 90.0 °C | 194 °F | |
| Flammability, UL94 | HB <br>@Thickness 3.18 mm |
HB <br>@Thickness 0.125 in |
|
| Oxygen Index | 18 % | 18 % |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Electrical Resistivity | >= 1.00e+15 ohm-cm | >= 1.00e+15 ohm-cm | |
| Surface Resistance | 1.00e+13 ohm | 1.00e+13 ohm | |
| Dielectric Constant | 2.5 <br>@Frequency 100 Hz |
2.5 <br>@Frequency 100 Hz |
|
| 2.5 <br>@Frequency 1e+6 Hz |
2.5 <br>@Frequency 1e+6 Hz |
||
| Dissipation Factor | 0.00040 <br>@Frequency 100 Hz |
0.00040 <br>@Frequency 100 Hz |
|
| 0.00040 <br>@Frequency 1e+6 Hz |
0.00040 <br>@Frequency 1e+6 Hz |
||
| Comparative Tracking Index | 500 V | 500 V |