Material Notes:
Chemical Name: Tris(3,5-di-tert-butyl-4-hydroxybenzyl) isocyanurateCAS NO.: 27676-62-6Molecular Formula: C48H69N3O6Property: It is one kind of multi-functional Antioxidant, with multiple functional groups. It is one kind of low toxic chemicals, and it can be used in food packing.Uses: It can be used in ABS resin, polyester, Nylon, PE, PS, PVC, PU, cellulose plastic and rubber. It can work with UV absorbent or phosphite ester to improve the stability.Dosage: 0.1-0.25%.Information Provided by Suqian Unitechem Co., Ltd.
Physical Properties Metric English Comments
Density <= 1.03 g/cc
<= 0.0372 lb/in³
Relative density
Volatiles <= 0.20 %
<= 0.20 %
Molecular Weight 784.1 g/mol
784.1 g/mol
Ash <= 0.10 %
<= 0.10 %
Thermal Properties Metric English Comments
Melting Point 218 - 223 °C
424 - 433 °F
Flash Point 289.4 °C
552.9 °F
Optical Properties Metric English Comments
Transmission, Visible >= 93 %
>= 93 %
425nm
>= 95 %
>= 95 %
500nm
Descriptive Properties Value Comments
Appearance White powder
Purity (%) >98