| Category | Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, Unreinforced |
| Manufacturer | |
| Trade Name | |
| Port | Ningbo port,China |
| Trade Terms | FOB, CFR, CIF |
| Payment Terms | L/C, T/T, Western Union |
| Download PDF | BASF Capron® 8202 NL Nylon 6 (Conditioned)
(discontinued **).pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.13 g/cc | 0.0408 lb/in³ | (DAM); ISO 1183 |
| Water Absorption | 1.6 % | 1.6 % | 24 hr. (DAM); ISO 62 |
| 9.5 % | 9.5 % | (Beginning DAM); ISO 62 | |
| Moisture Absorption at Equilibrium | 2.7 % | 2.7 % | 23°C/50% R.H. (Beginning DAM); ISO 62 |
| Viscosity Measurement | 48 | 48 | Formic Acid; ASTM D789 |
| Linear Mold Shrinkage | 0.012 cm/cm | 0.012 in/in | MD; ASTM Test |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength at Break | 60.0 MPa | 8700 psi | 0.2 in/min; ASTM D638 |
| Tensile Strength, Ultimate | 80.0 MPa @Temperature -40.0 °C |
11600 psi @Temperature -40.0 °F |
ASTM D638 |
| 80.0 MPa @Temperature -40.0 °C |
11600 psi @Temperature -40.0 °F |
ISO 527 | |
| Tensile Strength, Yield | 36.0 MPa | 5220 psi | 50 mm/min; ISO 527 |
| 36.0 MPa | 5220 psi | 2 in/min; ASTM D638 | |
| 21.0 MPa @Temperature 120 °C |
3050 psi @Temperature 248 °F |
ASTM D638 | |
| 21.0 MPa @Temperature 120 °C |
3050 psi @Temperature 248 °F |
ISO 527 | |
| 30.0 MPa @Temperature 80.0 °C |
4350 psi @Temperature 176 °F |
ASTM D638 | |
| 30.0 MPa @Temperature 80.0 °C |
4350 psi @Temperature 176 °F |
ISO 527 | |
| 110 MPa @Temperature -40.0 °C |
16000 psi @Temperature -40.0 °F |
ASTM D638 | |
| 110 MPa @Temperature -40.0 °C |
16000 psi @Temperature -40.0 °F |
ISO 527 | |
| Elongation at Break | >= 50 % | >= 50 % | 50 mm/min; Nominal; ISO 527 |
| >= 100 % | >= 100 % | 2 in/min; ASTM D638 | |
| 2.5 % @Temperature -40.0 °C |
2.5 % @Temperature -40.0 °F |
ASTM D638 | |
| Elongation at Yield | 16 % | 16 % | 50 mm/min; ISO 527 |
| 16 % | 16 % | 2 in/min; ASTM D638 | |
| 35 % @Temperature 80.0 °C |
35 % @Temperature 176 °F |
ASTM D638 | |
| 40 % @Temperature 120 °C |
40 % @Temperature 248 °F |
ASTM D638 | |
| Tensile Modulus | 0.970 GPa | 141 ksi | 1 mm/min; ISO 527 |
| Flexural Strength | 35.0 MPa | 5080 psi | ASTM D790 |
| 155 MPa @Temperature -40.0 °C |
22500 psi @Temperature -40.0 °F |
ASTM D790 | |
| Flexural Modulus | 0.740 GPa | 107 ksi | ASTM D790 |
| 3.66 GPa @Temperature -40.0 °C |
531 ksi @Temperature -40.0 °F |
ASTM D790 | |
| Izod Impact, Notched | NB | NB | ASTM D256 |
| 0.450 J/cm @Temperature -40.0 °C |
0.843 ft-lb/in @Temperature -40.0 °F |
ASTM D256 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Melting Point | 220 °C | 428 °F | 10 K/min (DAM) |
| 220 °C | 428 °F | (DAM); ASTM D3418 |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Additive | Unfilled | |
| Color | Natural | |
| Commercial Status (March 2007) | Active America | |
| FDA | 21 CFR 177.1500 | |
| Form | Pellets | |
| Impact Modified | No | |
| Injection molding | Processable | |
| Primary Processing Technique | Film Extrusion |