Axiall 8247 Clear 34 Rigid PVC, Extrusion, Clear 34

Category Polymer , Thermoplastic , Vinyl (PVC)
Manufacturer Axiall
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Axiall 8247 Clear 34 Rigid PVC, Extrusion, Clear 34.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Georgia Gulf 8247 Clear 34 is a rigid PVC pellet compound suited for applications where transparency is important. It is widely used for clear profiles such as furniture trim, shower door and protected jalousie windows. High impact vacuum formed sheet applications are also filled with 8247 Clear 34. Twin screw machines may be used to convert Georgia Gulf 8247 Clear 34. 8247 is characterized by excellent physical properties and easy processing. It contains UV inhibitor to retard deterioration. It is available in fiberboard boxes, railroad bulk hopper cars or bulk truckloads. It is available in a neutral pale green tint and is easily colored by concentrates at the machine.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Physical Properties Metric English Comments
Specific Gravity 1.32 g/cc
1.32 g/cc
ASTM D-792
Mechanical Properties Metric English Comments
Hardness, Rockwell R 112
112
ASTM D-785
Hardness, Shore D 79
79
ASTM D-2240
Tensile Strength, Yield 44.8 MPa
6500 psi
ASTM D-638
Tensile Modulus 2.62 GPa
380 ksi
ASTM D-638
Flexural Strength 81.4 MPa
11800 psi
ASTM D-790
Flexural Modulus 2.62 GPa
380 ksi
ASTM D-790
Izod Impact, Notched 6.41 J/cm

@Thickness 3.17 mm,
Temperature 23.0 °C
12.0 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
ASTM D-256
Tensile Impact Strength 187 kJ/m²
89.0 ft-lb/in²
ASTM D-1822
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 72.2 °C
162 °F
ASTM D-648
Flammability, UL94 V-0
V-0
Optical Properties Metric English Comments
Transmission, Visible 90 %
90 %
clear; thickness not quantified
Descriptive Properties Value Comments
Cell Classification 14443333
ASTM D-4216