Material Notes:
AA-BOND 428 is a two part, heat-resistant and low exotherm, epoxy adhesive formulation. It is a 100% solid epoxy adhesive, with superior chemical resistance and shear strength. AA-BOND 428 contains a thixotrophic agent which impedes thinning out of the material during heat cure when properly mixed and curedAppearance: AmberCure Type: Heat cure or Room TemperatureBenefits:Room temperature of heat cureTough enamel like cureBonds variety of substratesWeather resistant Mix Ratio by weight: 100:100/Resin:Hardener Substrates: Metals, glass, ceramics, wood and many plastics Typical Application: Staking components, bonding, laminating and repair applicationsInformation provided by Atom Adhesives
Physical Properties Metric English Comments
Specific Gravity 1.07 g/cc
1.07 g/cc
uncured
Solids Content 100 %
100 %
reactive, uncured
Mechanical Properties Metric English Comments
Hardness, Shore D 78
78
Shear Strength 20.0 MPa
2900 psi
Lap, Alum to Alum
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 163 °C
325 °F
Minimum Service Temperature, Air -60.0 °C
-76.0 °F
Glass Transition Temp, Tg 93.0 °C
199 °F
Processing Properties Metric English Comments
Cure Time 240 - 360 min

@Temperature 65.0 °C
4.00 - 6.00 hour

@Temperature 149 °F
1440 min

@Temperature 25.0 °C
24.0 hour

@Temperature 77.0 °F
Pot Life 60.0 min
60.0 min
uncured