Henkel Turco EA Stripper R 6955 GL Paint Remover

Category Fluid , Solvent
Manufacturer Henkel
Trade Name Turco
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Henkel Turco EA Stripper R 6955 GL Paint Remover.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Turco Stripper 6955 GL is an environmentally advantaged thixotropic paint remover activated by hydrogen peroxide. It was developed for effective stripping of such resistant finishes as epoxies, epoxy primers, polyurethanes, and similar catalyzed aircraft paints. Turco Stripper 6955 GL paint remover offers a significant advance in paint stripper technology. Offers a significant advance in paint stripper technology. Complies fully with the aircraft / aerospace NESHAP. Can be used on aluminum, mild steel, high strength steel, cadmium plated steel and titanium when used as directed.
Processing Properties Metric English Comments
Processing Temperature 23.0 °C
73.4 °F
Descriptive Properties Value Comments
Chemistry Peroxide activated, water-based
Consistency Liquid
Form Ready-to-Use
Substrate Aluminum
Ferrous
Non-Ferrous
Stainless Steel
Titanium