Ashley Polymers Ashlene® 528L-40G Nylon 66, 40% Glass Reinforced

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, 40% Glass Fiber Filled
Manufacturer Ashley Polymers
Trade Name Ashlene®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ashley Polymers Ashlene® 528L-40G Nylon 66, 40% Glass Reinforced.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
A general purpose 40% glass reinforced Nylon 66 resin.Data provided by the manufacturer
Physical Properties Metric English Comments
Density 1.46 g/cc
0.0527 lb/in³
ASTM D792
Water Absorption 0.70 %
0.70 %
ASTM D570
Linear Mold Shrinkage 0.0045 cm/cm
0.0045 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 120
120
ASTM D785
Tensile Strength, Yield 214 MPa
31000 psi
ASTM D638
Elongation at Break 2.0 %
2.0 %
ASTM D638
Flexural Strength 269 MPa
39000 psi
ASTM D790
Flexural Modulus 11.0 GPa
1600 ksi
ASTM D790
Izod Impact, Notched 1.28 J/cm
2.40 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Melting Point 251 °C
484 °F
ASTM D3418
Deflection Temperature at 0.46 MPa (66 psi) 254 °C
489 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 249 °C
480 °F
ASTM D648