Arlon Flexible Silicon Insulation with Fiberglass Substrate (56493F031)

Category Polymer , Thermoset , Filled/Reinforced Thermoset , Silicone
Manufacturer Arlon
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Arlon Flexible Silicon Insulation with Fiberglass Substrate (56493F031).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Side one - cured silicone rubber ,0.007 in. (0.18 mm) minimum: Substrate - Prime Coated 1564 Fiberglass, 0.017 in. (0.43 mm) nominal; Side two- cured silicone rubber, 0.007 in. (0.18 mm) minimum; 0.003 in. (0.08 mm) polyethylene interleave; overall thickness 0.031 in ±0.0025 (0.79 mm ± 0.063). Color: Blue-black. Weight: 1122 g/m² ± 102 (33.1 oz./yd.² ± 3.0). Shelf Life: 12 months from the date of manufacture. The shelf life is defined as the duration of time for which the product will meet the physical requirements outlined below. It does not guarantee the product’s usefulness in all applications. Flame Test Method: FTMS 191A; Method 5903. Maximum Flame and Glow Time: 25 seconds. Maximum Char Length: 7.62 cm (3 in).Information provided by the manufacturer, Arlon Silicone Technologies Division.
Mechanical Properties Metric English Comments
Hardness, Shore A 45 - 55
45 - 55
Tensile Strength, Ultimate 7.61 - 8.99 MPa
1100 - 1300 psi
Elongation at Break 300 - 500 %
300 - 500 %
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 232 °C
450 °F
Minimum Service Temperature, Air -97.8 °C
-144 °F
Electrical Properties Metric English Comments
Dielectric Strength >= 15.75 kV/mm
>= 400.0 kV/in