| Category | Polymer , Thermoset , Silicone , Silicone Rubber , Silicone, Molded, Glass Fiber Filled | 
| Manufacturer | Arlon | 
| Trade Name | |
| Port | Shanghai port,China | 
| Trade Terms | FOB, CFR, CIF | 
| Payment Terms | L/C, T/T, Western Union | 
| Download PDF | Arlon 56946C026 Silicone Rubber/Fiberglass Laminate.pdf  | 
          
| Price | EMAIL US sales@lookpolymers.com | 
| Physical Properties | Metric | English | Comments | 
|---|---|---|---|
| Specific Gravity | 1.33 g/cc | 1.33 g/cc | silicone property; Arlon SQA-TMS-024 | 
| Thickness | 152 microns | 6.00 mil | side 1; Arlon SQA-TMS-003 | 
| 152 microns | 6.00 mil | side 2; Arlon SQA-TMS-003 | |
| 406 microns | 16.0 mil | substrate; Arlon SQA-TMS-003 | |
| 711 microns | 28.0 mil | overall; Arlon SQA-TMS-003 | 
| Mechanical Properties | Metric | English | Comments | 
|---|---|---|---|
| Hardness, Shore A | 55 | 55 | silicone property; ASTM D2240 | 
| Tensile Strength, Ultimate | 7.93 MPa | 1150 psi | silicone property; ASTM D412 | 
| Elongation at Break | 500 % | 500 % | silicone property; ASTM D412 | 
| Adhesive Bond Strength | 0.0710 MPa | 10.3 psi | Arlon SQA-TMS-011 | 
| Thermal Properties | Metric | English | Comments | 
|---|---|---|---|
| Maximum Service Temperature, Air | 232 °C | 450 °F | |
| Minimum Service Temperature, Air | -56.7 °C | -70.0 °F | 
| Electrical Properties | Metric | English | Comments | 
|---|---|---|---|
| Dielectric Strength | 19.7 kV/mm | 500 kV/in | ASTM D149 | 
| Processing Properties | Metric | English | Comments | 
|---|---|---|---|
| Cure Time |           120           min           @Temperature 204 °C  | 
                  2.00           hour           @Temperature 400 °F  | 
        |
|           15.0           min           @Pressure 0.345 MPa, Temperature 121 °C  | 
                  0.250           hour           @Pressure 50.0 psi, Temperature 250 °F  | 
        ||
| Shelf Life |           6.00           Month           @Temperature 23.9 °C  | 
                  6.00           Month           @Temperature 75.0 °F  | 
        
| Descriptive Properties | Value | Comments | 
|---|---|---|
| Color | Brown |