Material Notes:
Properties: VICOTE 701-707 grades are specially developed powder coatings. They are available in various average particle sizes from 10 - 50 microns. The powders are off-white in color and are available in various melt viscosities depending on the film thickness and level of melt flow required. Typical film thicknesses range from < 100 microns up to 500 microns. Film thicknesses above 1 mm are possible by building up the coating thickness by the hot flocking technique. Like other non-coating grades of VICTREXPEEK polymer, VICOTE Coatings are thermoplastic in nature and exhibit flow above the melt temperature. When processed using the correct guidelines, the coatings will exhibit the excellent properties that VICTREX PEEK polymer is renowned for. High continuous use temperature of 260°C Excellent wear, abrasion and cut through resistance at these high temperatures Excellent chemical and radiation resistance Low level of extractables Hydrolysis resistant Inherently flame retardantAll information provided by Victrex.
Physical Properties Metric English Comments
Density 1.32 g/cc
0.0477 lb/in³
ISO 1183
Thermal Properties Metric English Comments
Melting Point 343 °C
649 °F
DSC
Glass Transition Temp, Tg 143 °C
289 °F
DSC
UL RTI, Electrical 260 °C
500 °F
UL746B
Processing Properties Metric English Comments
Drying Temperature 120 °C
248 °F
overnight before use
150 °C

@Time 10800 sec
302 °F

@Time 3.00 hour
Descriptive Properties Value Comments
Konig Hardness 200 seconds
BS EN ISO 1522