| Category | Polymer , Thermoset , Silicone , Silicone Rubber , Silicone, Molded, Glass Fiber Filled |
| Manufacturer | Arlon |
| Trade Name | |
| Port | Shanghai port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | Arlon 55143R060 Silicone Rubber/Fiberglass Laminate.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.35 g/cc | 1.35 g/cc | silicone property; Arlon SQA-TMS-024 |
| Thickness | 457 microns | 18.0 mil | substrate; Arlon SQA-TMS-003 |
| 533 microns | 21.0 mil | side 1; Arlon SQA-TMS-003 | |
| 533 microns | 21.0 mil | side 2; Arlon SQA-TMS-003 | |
| 1520 microns | 60.0 mil | overall; Arlon SQA-TMS-003 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Shore A | 60 | 60 | silicone property; ASTM D2240 |
| Tensile Strength, Ultimate | 5.52 MPa | 800 psi | silicone property; ASTM D412 |
| Elongation at Break | 225 % | 225 % | silicone property; ASTM D412 |
| Tear Strength | 15.8 kN/m | 90.0 pli | Die B; silicone property; ASTM D624 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Maximum Service Temperature, Air | 232 °C | 450 °F | |
| Minimum Service Temperature, Air | -56.7 °C | -70.0 °F | |
| UL RTI, Electrical | 200 °C | 392 °F | |
| UL RTI, Mechanical without Impact | 200 °C | 392 °F |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Dielectric Strength | 15.7 kV/mm | 400 kV/in | ASTM D149 |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Cure Time | 120 min @Temperature 204 °C |
2.00 hour @Temperature 400 °F |
|
| Shelf Life | 60.0 Month @Temperature 23.9 °C |
60.0 Month @Temperature 75.0 °F |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Color | Red |