Dymax 957 Potting and Encapsulation Adhesive

Category Polymer , Adhesive , Thermoset
Manufacturer Dymax Corporation
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dymax 957 Potting and Encapsulation Adhesive.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
High Performance Light-Curing Adhesives and Coatings for Electronic AssemblyDymax 957 Potting and Encapsulation AdhesiveDesigned to adhere to a wide variety of materials, high strength. Cure Type: UV or Heat
Physical Properties Metric English Comments
Viscosity 650 cP
650 cP
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 24.1 MPa
3500 psi
Processing Properties Metric English Comments
Cure Time <= 0.250 min
<= 0.00417 hour
Descriptive Properties Value Comments
Cure Depth 0.1 in.