Material Notes:
Characteristics:Self lubricating ( graphite modified )Good glide propertiesGood sealing propertiesMedium or low mechanical strengthUnsuitable for electrical applicationGlossy surfaceThermal conductivityColor-gray blackSoft flow Applications:SealsSelf lubricating parts / housings , etc. Information provided by Amity Thermosets Limited
Physical Properties Metric English Comments
Density 1.55 - 1.62 g/cc
0.0560 - 0.0585 lb/in³
Molding; IS 867-1963
Apparent Bulk Density 0.750 - 0.840 g/cc
0.0271 - 0.0303 lb/in³
IS 867-1963
Water Absorption 0.20 - 0.30 %
0.20 - 0.30 %
IS 13411-1993
Linear Mold Shrinkage 0.0035 - 0.0050 cm/cm
0.0035 - 0.0050 in/in
IS 13411-1992
Mechanical Properties Metric English Comments
Tensile Strength at Break 40.0 - 50.0 MPa
5800 - 7250 psi
5 mm/min.; IS 867-1963
Shear Strength 55.0 - 60.0 MPa
7980 - 8700 psi
IS 867-1963
Izod Impact, Notched 0.220 - 0.320 J/cm
0.412 - 0.599 ft-lb/in
IS 13411-1992
Processing Properties Metric English Comments
Mold Temperature 160 - 170 °C
320 - 338 °F
Injection Pressure 15.68 - 34.3 MPa
2274 - 4970 psi
Mold Pressure
Cure Time 0.417 - 0.667 min
0.00694 - 0.0111 hour
per mm
Shelf Life 12.0 Month
12.0 Month
10-25°C