SGL Carbon Group SIGRAFIL C® C30 S009 GLY Staple Carbon Fiber, Glycerine Sizing

Category Carbon , Carbon Fiber , Other Engineering Material , Composite Fibers
Manufacturer SGL Carbon Group
Trade Name SIGRAFIL C®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SGL Carbon Group SIGRAFIL C® C30 S009 GLY Staple Carbon Fiber, Glycerine Sizing.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
In its precision cut staple form SIGRAFIL C is a superior free-flowing material suitable for low and high temperature thermoplastic injection-molding processes. It is also an excellent way of making plastics or other non-conductive bulk materials electrically conductive e.g. glues, resin systems, and specialty paper. Further important uses include fuel cells, cement reinforcement and applications where enhanced chemical resistance is needed. The sizing type and surface treatment can be tailored for individual end uses.Information provided by SGL Carbon Group
Physical Properties Metric English Comments
Density 1.82 g/cc
0.0658 lb/in³
Fiber Density
Filament Diameter 7.0 µm
7.0 µm
Mechanical Properties Metric English Comments
Tensile Strength at Break 3800 MPa
551000 psi
ASTM D3379-96
Elongation at Break 1.2 - 1.6 %
1.2 - 1.6 %
ASTM D3379-75
Modulus of Elasticity 240 GPa
34800 ksi
ASTM D3379-96
Electrical Properties Metric English Comments
Volume Resistivity 0.0013 ohm-cm
0.0013 ohm-cm
Descriptive Properties Value Comments
Carbon Content, wt % >95
Mean Fiber Length, mm 9
Chopped
Sizing Content, % by weight 1.5 - 6.5