Material Notes:
DuPont™ Elvax® 210W is an ethylene-vinyl acetate copolymer resin containing an anti-blocking additive for use in industrial applications. This resin is supplied in pellet form and to prevent the pellets from blocking, low levels of a (W) amide additive is added to the polymer. Additions: antiblock.Applications:Elvax® 210W resins can be used for the following applications: adhesives, sealants, and wax blends.Information provided by DuPont™
Physical Properties Metric English Comments
Density 0.951 g/cc
0.0344 lb/in³
ASTM D792-ISO 1183
Vinyl Acetate Content 28 %
28 %
Melt Flow 400 g/10 min

@Load 2.16 kg,
Temperature 190 °C
400 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238, ISO 1133
Mechanical Properties Metric English Comments
Hardness, Shore A 62
62
ASTM D2240-ISO 868
Thermal Properties Metric English Comments
Ring & Ball Softening Point 82.0 °C
180 °F
ASTM E28
Descriptive Properties Value Comments
Cloud Point in Paraffin Wax, °C 66
10% Elvax® in fully refined paraffin wax, 146 AMP. Incompatible at temperatures up to 177°C.