Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Akro-Plastic Akromid® B3 GF 35 (2473) PA 6 Conditioned, 35% Glass Filled

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, 40% Glass Fiber Filled
Manufacturer Akro-Plastic
Trade Name Akromid®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Akro-Plastic Akromid® B3 GF 35 (2473) PA 6 Conditioned, 35% Glass Filled.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
AKROMID® B (Polyamide 6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperatures as well as easy processing. AKROMID® B is an engineering plastic compound that allows a broad range of possible applications. On the basis of these standard types, we are able to develop individual compounds for special application needs.Information from Akro-Plastic
Physical Properties Metric English Comments
Density 1.41 g/cc
0.0509 lb/in³
ISO 1183
Filler Content 35 %
35 %
ISO 1172
Water Absorption 1.8 - 2.1 %

@Temperature 70.0 °C
1.8 - 2.1 %

@Temperature 158 °F
62% r.h., Humidity; ISO 62
Water Absorption at Saturation 5.9 - 6.5 %

@Time 82800 sec
5.9 - 6.5 %

@Time 23.0 hour
ISO 62
Linear Mold Shrinkage, Flow 0.0010 cm/cm
0.0010 in/in
ISO 294-4
Linear Mold Shrinkage, Transverse 0.0080 cm/cm
0.0080 in/in
ISO 294-4
Mechanical Properties Metric English Comments
Tensile Strength at Break 120 MPa
17400 psi
5 [mm/min]; ISO 527-1/2
Elongation at Break 5.0 %
5.0 %
5 [mm/min]; ISO 527-1/2
Tensile Modulus 7.30 GPa
1060 ksi
1[mm/min]; ISO 527-1/2
Charpy Impact Unnotched 11.0 J/cm²

@Temperature 23.0 °C
52.3 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eU
Charpy Impact, Notched 2.10 J/cm²

@Temperature 23.0 °C
9.99 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eA
Thermal Properties Metric English Comments
Melting Point 220 °C
428 °F
ISO 11357-1/3
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+10 ohm-cm
1.00e+10 ohm-cm
IEC 60093
Surface Resistance 1.00e+10 ohm
1.00e+10 ohm
IEC 60093