Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

SABIC Innovative Plastics Valox® 830 PBT

Category Polymer , Thermoplastic , Polyester, TP , Polybutylene Terephthalate (PBT)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name Valox®
Port Ningbo port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF SABIC Innovative Plastics Valox® 830 PBT.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
30% GR PBTP, excellent surface finish. Typical applications are hot air gun housing assemblies, industrial glue guns, appliance housings and handles.
Physical Properties Metric English Comments
Specific Gravity 1.54 g/cc
1.54 g/cc
ASTM D792
Water Absorption 0.060 %

@Time 86400 sec
0.060 %

@Time 24.0 hour
ASTM D570
Linear Mold Shrinkage, Flow 0.0030 - 0.0050 cm/cm

@Thickness 1.50 - 3.20 mm
0.0030 - 0.0050 in/in

@Thickness 0.0591 - 0.126 in
SABIC Method
0.0050 - 0.0080 cm/cm

@Thickness 3.20 - 4.60 mm
0.0050 - 0.0080 in/in

@Thickness 0.126 - 0.181 in
SABIC Method
Linear Mold Shrinkage, Transverse 0.0040 - 0.0060 cm/cm

@Thickness 1.50 - 3.20 mm
0.0040 - 0.0060 in/in

@Thickness 0.0591 - 0.126 in
SABIC Method
0.0060 - 0.0090 cm/cm

@Thickness 3.20 - 4.60 mm
0.0060 - 0.0090 in/in

@Thickness 0.126 - 0.181 in
SABIC Method
Mechanical Properties Metric English Comments
Hardness, Rockwell R 119
119
ASTM D785
Tensile Strength at Break 106 MPa
15400 psi
Type I, 5 mm/min; ASTM D638
Tensile Strength, Yield 103 MPa
14900 psi
Type I, 5 mm/min; ASTM D638
Flexural Strength 172 MPa
24900 psi
1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 6.89 GPa
999 ksi
1.3 mm/min, 50 mm span; ASTM D790
Izod Impact, Notched 0.800 J/cm
1.50 ft-lb/in
ASTM D256
Izod Impact, Unnotched 6.40 J/cm
12.0 ft-lb/in
ASTM D4812
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 25.2 µm/m-°C

@Temperature -40.0 - 40.0 °C
14.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
25.2 µm/m-°C

@Temperature 60.0 - 138 °C
14.0 µin/in-°F

@Temperature 140 - 280 °F
ASTM E 831
Deflection Temperature at 0.46 MPa (66 psi) 221 °C

@Thickness 6.40 mm
430 °F

@Thickness 0.252 in
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 193 °C

@Thickness 6.40 mm
379 °F

@Thickness 0.252 in
unannealed; ASTM D648
UL RTI, Electrical 120 °C
248 °F
UL 746B
UL RTI, Mechanical without Impact 120 °C
248 °F
UL 746B
Flammability, UL94 HB

@Thickness 1.47 mm
HB

@Thickness 0.0579 in
UL 94
Electrical Properties Metric English Comments
Volume Resistivity 4.00e+16 ohm-cm
4.00e+16 ohm-cm
ASTM D257
Dielectric Constant 3.5

@Frequency 1.00e+6 Hz
3.5

@Frequency 1.00e+6 Hz
ASTM D150
3.6

@Frequency 100 Hz
3.6

@Frequency 100 Hz
ASTM D150
Dielectric Strength 20.8 kV/mm

@Thickness 3.20 mm
528 kV/in

@Thickness 0.126 in
in air; ASTM D149
24.8 kV/mm

@Thickness 1.60 mm
630 kV/in

@Thickness 0.0630 in
in oil; ASTM D149
Dissipation Factor 0.0020

@Frequency 100 Hz
0.0020

@Frequency 100 Hz
ASTM D150
0.020

@Frequency 1.00e+6 Hz
0.020

@Frequency 1.00e+6 Hz
ASTM D150
Arc Resistance 60 - 120 sec
60 - 120 sec
Tungsten; ASTM D495
Comparative Tracking Index 250 - 400 V
250 - 400 V
UL 746A
Hot Wire Ignition, HWI >= 120 sec
>= 120 sec
UL 746A
High Amp Arc Ignition, HAI 15 - 30 arcs
15 - 30 arcs
UL 746A
High Voltage Arc-Tracking Rate, HVTR 25.4 - 80.0 mm/min
1.00 - 3.15 in/min
UL 746A
Descriptive Properties Value Comments
Specific Volume 0.67cm^3/g
ASTM D792