Goodfellow Zirconium 56.5/Vanadium 43.5 Alloy

Category Metal , Nonferrous Metal , Zirconium Alloy
Manufacturer Goodfellow
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Goodfellow Zirconium 56.5/Vanadium 43.5 Alloy.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Information provided by Goodfellow.
Thermal Properties Metric English Comments
Melting Point 1390 °C
2530 °F
Component Elements Properties Metric English Comments
Vanadium, V 43.5 %
43.5 %
Zirconium, Zr 56.5 %
56.5 %