Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Advanced Elastomer Systems Santoprene® 221-73 W175 Thermoplastic Rubber  (discontinued **)

Category Polymer , Thermoplastic , Elastomer, TPE , Thermoplastic Elastomer, Melt-Processible Rubber
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Advanced Elastomer Systems Santoprene® 221-73 W175 Thermoplastic Rubber  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
A colorable thermoplastic UV grade elastomer designed for thin wall extrusion applications with good fluid resistance, formulated to replace thermoset elastomers such as EPDM, polychloroprene, and chlorosulfonated polyethylene. It can be processed using extrusion or other melt processing techniques.Key Features: Dielectric constant 2.3, dielectric strength at 3.17 mm (125 mil), 19.6 kV/mm (500 v/mil); Continuous temperature rating 1000 hrs. @ 135°C (275°F); Excellent flex fatigue resistance; Excellent ozone resistance; Excellent mechanical properties retention after UV exposure; Extrudes thin sections with excellent definition (down to 0.33 mm [1.3"] radius). Long runs with minimal build-up of material on screen packs or narrow die sections.Additional processing comments: This thermoplastic rubber is a shear-dependent material that can be processed on conventional thermoplastic equipment for injection molding, extrusion, or blow molding. For extrusion, a general purpose screw with a compression ratio of 2.5 to 3.0 is recommended. Material can be recycled. SANTOPRENE rubber is incompatible with acetal and PVC.Values below are for injection molded plaques, side gated, 82.6 mm x 117.5 mm x 3.0 mm. Tensile properties measured across flow. Data provided by Advanced Elastomer Systems.Advanced Elastomer Systems is now a part of ExxonMobil. This grade was removed from the Advanced Elastomers Systems standard product line before the ExxonMobil acquisiton.
Physical Properties Metric English Comments
Density 0.960 g/cc
0.0347 lb/in³
TPE-0105 (ASTM D792)
Mechanical Properties Metric English Comments
Hardness, Shore A 73
73
5 Second; TPE-0169 (ASTM D 2240)
Tensile Strength, Ultimate 8.40 MPa
1220 psi
TPE-0153 (ASTM D 412)
Elongation at Break 500 %
500 %
TPE-0153 (ASTM D 412)
100% Modulus 0.00340 GPa
0.493 ksi
TPE-0153 (ASTM D 412)
Tear Strength 28.0 kN/m
160 pli
28 kN/m at 23°C. Value at 100°C is 13 kN/m. TPE-0056 (ASTM D 624)
Compression Set 29 %
29 %
23°C, 168 hrs.; TPE-0016 (ASTM D 412)
42 %

@Temperature 100 °C
42 %

@Temperature 212 °F
168 hrs.; TPE-0016 (ASTM D 412)
Tensile Set 14 %
14 %
23°C, 168 hrs.; TPE-0053 (ASTM D 412)
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 135 °C
275 °F
Continuous temperature Rating, 1000 hours
Brittleness Temperature <= -60.0 °C
<= -76.0 °F
TPE-0089 (ASTM D 746)
Electrical Properties Metric English Comments
Dielectric Constant 2.3
2.3
Frequency not specified
Dielectric Strength 19.6 kV/mm

@Thickness 3.17 mm
498 kV/in

@Thickness 0.125 in
Processing Properties Metric English Comments
Processing Temperature 177 - 232 °C
351 - 450 °F
Drying Temperature 82.0 °C
180 °F
Desiccant drying for 3 hours recommended
Dry Time 3 hour