Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Axion Polymers Axplas® PS04 0000 Mixed Polystyrene Granules with FR

Category Polymer , Renewable/Recycled Polymer , Thermoplastic , Polystyrene (PS) , Polystyrene, Flame Retardant
Manufacturer Axion Polymers
Trade Name Axplas®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Axion Polymers Axplas® PS04 0000 Mixed Polystyrene Granules with FR.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
The PS04 series of clean, mixed polystyrene granular chips offers a low-cost option for manufacturers to add post-consumer, engineering polymers to a wide range of products. The polymer mix includes a high proportion of styrenic thermoplastics including PS, HIPS, ABS and traces of PC/ABS.The Axplas® PS04 product is produced under strict quality control procedures and is consistently free from metal and other contaminants. The origin of the material means that this granular fraction contains a higher level of brominated flame retardants than our fully compounded resins - a factor which some users see as a potential benefit in the end-use application of the material.Produced from 100% post-consumer raw materials, this product fits closely with Axion's other recycled resin grades and offers the same set of user benefits, including:Huge savings in CO2 impactAppeals to 'greener' customersCost-down on raw materialThe Axplas PS04 chips have a particle size range with 90% of mass between 2-8 mm.Information provided by Axion Recycling
Physical Properties Metric English Comments
Bulk Density 0.600 g/cc
0.0217 lb/in³
Density 1.14 g/cc
0.0412 lb/in³
Melt Index of Compound 8.0 g/10 min

@Load 5.00 kg,
Temperature 200 °C
8.0 g/10 min

@Load 11.0 lb,
Temperature 392 °F
Mechanical Properties Metric English Comments
Tensile Strength, Yield 30.0 MPa
4350 psi
Izod Impact, Unnotched (ISO) 5.00 kJ/m²
2.38 ft-lb/in²
Descriptive Properties Value Comments
Br Level 0.08
Visual Appearance Mixed Dark Colored
Users viewing this material also viewed the following: