| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.27 g/cc | 0.0459 lb/in³ | ASTM D792 |
| Linear Mold Shrinkage | 0.0010 cm/cm | 0.0010 in/in | MD; ASTM D955 |
| Melt Flow | 0.90 g/10 min | 0.90 g/10 min | ASTM D1238 |
| Ash | 30 % | 30 % | ASTM D2584 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Rockwell R | 107 | 107 | ASTM D785 |
| Tensile Strength at Break | 89.98 MPa | 13050 psi | ASTM D638 |
| Tensile Strength, Yield | 89.98 MPa | 13050 psi | ASTM D638 |
| Elongation at Break | 4.0 % | 4.0 % | ASTM D638 |
| Elongation at Yield | 3.0 % | 3.0 % | ASTM D638 |
| Tensile Modulus | 5.199 GPa | 754.1 ksi | ASTM D638 |
| Flexural Strength | 126.0 MPa | 18270 psi | ASTM D790 |
| Flexural Modulus | 8.1986 GPa | 1189.1 ksi | ASTM D790 |
| Izod Impact, Notched | 0.694 J/cm | 1.30 ft-lb/in | ASTM D256 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Deflection Temperature at 0.46 MPa (66 psi) | 102 °C | 216 °F | ASTM D648 |
| Deflection Temperature at 1.8 MPa (264 psi) | 95.0 °C | 203 °F |