Material Notes:
Tungsten key properties: Very high density, High oxidation resistance, Highest melting point of all metals, Lowest vapor pressure of all metals, Highest elasticity modulus of the all metals, Hardest pure metal, Excellent high temperature strength characteristics, High hardness, Resistive to thermal stress, High thermal conductivity, Low thermal expansion, Superior chemical inertness, is not attacked by nitric, hydrofluoric, or sulphuric acid solutionsTungsten main applications domains: Inert gas welding electrodes, Metal evaporation work, X-ray targets, Windings and heating elements for electric furnaces, Electroplating, As tungsten yarn, it is used for reinforcement in metal, ceramic and plastic compositesInformation provided by Acerde
Physical Properties Metric English Comments
Density 19.25 g/cc
0.6955 lb/in³
Mechanical Properties Metric English Comments
Tensile Modulus 411 GPa
59600 ksi
Flexural Strength 610 MPa
88500 psi
Thermal Properties Metric English Comments
CTE, linear 4.50 µm/m-°C

@Temperature <=1000 °C
2.50 µin/in-°F

@Temperature <=1830 °F
Melting Point 3422 °C
6192 °F
Electrical Properties Metric English Comments
Electrical Resistivity 0.00000530 ohm-cm

@Temperature 20.0 °C
0.00000530 ohm-cm

@Temperature 68.0 °F