R70-058 Styrene-based Biomedical Elastomer

Category Polymer , Thermoplastic , Elastomer, TPE , Styrenic TPE
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF R70-058 Styrene-based Biomedical Elastomer.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Physical Properties Metric English Comments
Specific Gravity 0.940 g/cc
0.940 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 70
70
ASTM D2240
Tensile Strength, Ultimate 14.3 MPa
2080 psi
ASTM D412
Tensile Strength, Yield 2.07 MPa
300 psi
at 100%; ASTM D412
Elongation at Break 660 %
660 %
ASTM D412
Tear Strength 21.0 kN/m
120 pli
die B; ASTM D624
Compression Set 55 %
55 %
ASTM D395