| Category | Carbon , Carbon Fiber , Other Engineering Material , Composite Fibers |
| Manufacturer | Zoltek |
| Trade Name | Panex 35® |
| Port | Ningbo port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | Zoltek Panex 35® Tow Weave Carbon Fiber Fabrics.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.81 g/cc | 0.0654 lb/in³ | |
| Filament Diameter | 7.2 µm | 7.2 µm | |
| Thickness | 1400 microns | 55.1 mil | |
| 2360 microns | 92.9 mil |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength, Ultimate | 4137 MPa | 600000 psi | |
| Tensile Modulus | 242 GPa | 35100 ksi |
| Component Elements Properties | Metric | English | Comments |
|---|---|---|---|
| Carbon, C | 95 % | 95 % |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Electrical Resistivity | 0.00155 ohm-cm | 0.00155 ohm-cm |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Areal Weights, g/m2 | 1640 | |
| 950 | ||
| Construction | Plain, Twill, Satin Weaves | |
| Filament Count | 50000 | |
| Roll Length, m | 25 | |
| Width, mm | 1270 | |
| Yarn | Zoltek Panex 35® 50k Continuous Tow |