Abatron AboWeld 48-33/AboCure 48-33 Epoxy

Category Polymer , Adhesive , Thermoset , Epoxy
Manufacturer Abatron
Trade Name AboWeld
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Abatron AboWeld 48-33/AboCure 48-33 Epoxy.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Data provided by the manufacturer, Abatron, Inc. Most versatile Abatron "VR" Epoxy thixotropic paste. White/black blend and other colors. Shelf life is 12+ months.Processing: 1/1 ratio. Pot life: 1-2 hrs.Applications: All-purpose adhesive, insulating filler, and patching compound.
Mechanical Properties Metric English Comments
Hardness, Shore D 80
80
Typical value for Abatron "VR" Epoxies.
Tensile Strength, Ultimate 55.0 MPa
7980 psi
Typical value for Abatron "VR" Epoxies.
Compressive Yield Strength 62.0 MPa
8990 psi
Typical value for Abatron "VR" Epoxies.
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 100 - 110 °C
212 - 230 °F
Heat distortion temperature