Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Abatron AboCast 8103-28 High-Performance Dielectric Epoxy

Category Polymer , Thermoset , Epoxy , Epoxy, Cast, Unreinforced
Manufacturer Abatron
Trade Name AboCast
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Abatron AboCast 8103-28 High-Performance Dielectric Epoxy.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
AboCast 8103-28 is a dielectric in/outdoor epoxy system with superior arc-track resistance, high voltage and heat resistance, low ash and ion content, and it is chlorine-free. This system has high heat conductivity, low thermal expansion, and negligible shrinkage.
Mechanical Properties Metric English Comments
Tensile Strength at Break 49.9 MPa
7240 psi
Elongation at Break 1.34 %
1.34 %
Tensile Modulus 6.76 GPa
981 ksi
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 126 °C
259 °F
Deflection Temp at unknown load
Electrical Properties Metric English Comments
Volume Resistivity 3.00e+13 ohm-cm
3.00e+13 ohm-cm
Dielectric Constant 4.0

@Frequency 60.0 Hz,
Temperature 23.0 °C
4.0

@Frequency 60.0 Hz,
Temperature 73.4 °F
4.9

@Frequency 60.0 Hz,
Temperature 100 °C
4.9

@Frequency 60.0 Hz,
Temperature 212 °F
5.6

@Frequency 60.0 Hz,
Temperature 150 °C
5.6

@Frequency 60.0 Hz,
Temperature 302 °F
Dielectric Strength 15.4 kV/mm
390 kV/in
S/T
Dissipation Factor 0.027

@Frequency 60.0 Hz,
Temperature 23.0 °C
0.027

@Frequency 60.0 Hz,
Temperature 73.4 °F
0.098

@Frequency 60.0 Hz,
Temperature 100 °C
0.098

@Frequency 60.0 Hz,
Temperature 212 °F
0.142

@Frequency 60.0 Hz,
Temperature 150 °C
0.142

@Frequency 60.0 Hz,
Temperature 302 °F
Processing Properties Metric English Comments
Cure Time 120 min

@Temperature 100 - 120 °C
2.00 hour

@Temperature 212 - 248 °F
120 - 240 min

@Temperature 120 - 160 °C
2.00 - 4.00 hour

@Temperature 248 - 320 °F
optional
Pot Life 30 min

@Temperature 80.0 °C
30 min

@Temperature 176 °F
>= 480 min

@Temperature 25.0 °C
>= 480 min

@Temperature 77.0 °F
Descriptive Properties Value Comments
Arc-Track Free (min) > 2000
2.5 KV
Color Gray or Custom
Parts by Weight (pbw) 100
Part A
17.6
Part B
Thermal Shock Resistance Scale 0 (poor) to 10 (excellent)
Users viewing this material also viewed the following: