Aaron Industries AAROPRENE® GFN 6613 Glass Filled Nylon 6/6

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, 10% Glass Fiber Filled
Manufacturer Aaron Industries Corporation
Trade Name AAROPRENE® GFN
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Aaron Industries AAROPRENE® GFN 6613 Glass Filled Nylon 6/6.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
AAROPRENE® GFN & MFN 6600 Series Reinforced CompoundsColor may be specified.
Physical Properties Metric English Comments
Specific Gravity 1.23 g/cc
1.23 g/cc
ASTM D792
Filler Content 13 %
13 %
Glass; ASTM D2584
Linear Mold Shrinkage 0.0050 cm/cm
0.0050 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength 102 MPa
14800 psi
ASTM D638
Flexural Modulus 4.83 GPa
700 ksi
ASTM D790
Izod Impact, Notched 0.534 J/cm
1.00 ft-lb/in
ASTM D256