Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

3M Scotch® 70 Self-Fusing Silicone Rubber Electrical Tape

Category Polymer , Adhesive
Manufacturer 3M
Trade Name Scotch®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M Scotch® 70 Self-Fusing Silicone Rubber Electrical Tape.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Scotch® 24 Brand 70 Silicone Rubber Electrical Tape is a high-temperature arc and track resistance tape composed of self-fusing, inorganic silicone rubber and easy-tear and easy-strip liner.Information provided by 3M
Physical Properties Metric English Comments
Thickness 305 microns
12.0 mil
Mechanical Properties Metric English Comments
Tensile Strength at Break 6.89 MPa
999 psi
ASTM D1000
Elongation at Break 450 %
450 %
ASTM D1000
Electrical Properties Metric English Comments
Dielectric Constant 2.51

@Temperature 150 °C
2.51

@Temperature 302 °F
ASTM D150
2.6

@Temperature 130 °C
2.6

@Temperature 266 °F
ASTM D150
2.89

@Temperature 90.0 °C
2.89

@Temperature 194 °F
ASTM D150
3.03

@Temperature 23.0 °C
3.03

@Temperature 73.4 °F
ASTM D150
Dielectric Strength 34.4 kV/mm
875 kV/in
ASTM D1000
Dissipation Factor 0.50

@Temperature 130 °C
0.50

@Temperature 266 °F
ASTM D150
0.70

@Temperature 150 °C
0.70

@Temperature 302 °F
ASTM D150
Arc Resistance 60 sec
60 sec
ASTM D495
Descriptive Properties Value Comments
Appearance Sky Blue Gray