Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

ALIMEX 7075 T651/T652 Aluminum Alloy Rolled

Category Metal , Nonferrous Metal , Aluminum Alloy , 7000 Series Aluminum Alloy
Manufacturer ALIMEX GmbH
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ALIMEX 7075 T651/T652 Aluminum Alloy Rolled.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Rolled aluminium material according to DIN EN standard. Information provided by ALIMEX GmbHSolution heat treated, stress-relieved by stretching a controlled amount then artificially aged. / Solution heat treated, stress-relieved by compressing to produce a permanent set of 1% to 5% and then artificially aged.
Physical Properties Metric English Comments
Density 2.801 g/cc
0.1012 lb/in³
Mechanical Properties Metric English Comments
Hardness, Brinell 105 - 160
105 - 160
Tensile Strength, Ultimate 360 - 545 MPa
52200 - 79000 psi
Rm
Tensile Strength, Yield 260 - 470 MPa

@Strain 0.200 %
37700 - 68200 psi

@Strain 0.200 %
Elongation at Break <= 8.0 %
<= 8.0 %
Modulus of Elasticity 70.0 GPa
10200 ksi
Thermal Properties Metric English Comments
CTE, linear 23.4 µm/m-°C

@Temperature 20.0 °C
13.0 µin/in-°F

@Temperature 68.0 °F
Thermal Conductivity 130.0 - 160.0 W/m-K
902.2 - 1110 BTU-in/hr-ft²-°F
Electrical Properties Metric English Comments
Electrical Resistivity 0.00000435 - 0.00000526 ohm-cm
0.00000435 - 0.00000526 ohm-cm
Descriptive Properties Value Comments
Corrosion Resistance Insufficient
Machinability Good
Protective Anodizing Satisfactory, not decorative
Welding Properties (WIG, MIG) Less Suitable
Users viewing this material also viewed the following: