3M FM29G Indoor UL Recognized Clear Polyester Overlaminate Label Products

Category Polymer , Adhesive
Manufacturer 3M
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M FM29G Indoor UL Recognized Clear Polyester Overlaminate Label Products.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
3M™ Indoor UL Recognized Clear Polyester Overlaminate Label Products are durable, high performance materials that offer excellent thermal stability and moisture resistance. These polyester overlaminate labels utilize 3M™ Adhesive P1212, which is a high clarity general purpose acrylic emulsion that exhibits good initial tack, excellent die cutting properties, minimal cold flow, and good UV resistance.Information provided by 3M
Physical Properties Metric English Comments
Thickness 50.8 microns
2.00 mil
Liner
76.2 microns
3.00 mil
Facestock
Mechanical Properties Metric English Comments
Peel Strength 0.526 kN/m
3.00 pli
180° Peel 12"/min, 1" wide sample; TLMI Method
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 49.0 °C
120 °F
Service
125 °C
257 °F
Application
Minimum Service Temperature, Air -29.0 °C
-20.2 °F
Application
5.00 °C
41.0 °F
Service
Descriptive Properties Value Comments
Adhesive Type P1212 Perm 18
Liner Clear Polypropylene Liner