3M 9415PC Repositionable Tape

Category Polymer , Adhesive
Manufacturer 3M
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M 9415PC Repositionable Tape.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
3M™ Repositionable Tapes are double coated tapes that are ideal for applications where one or both parts need to be repositioned or removed easily.Information provided by 3M
Physical Properties Metric English Comments
Thickness 25.4 microns
1.00 mil
Carrier
50.8 microns
2.00 mil
Tape
142 microns
5.60 mil
Liner
Mechanical Properties Metric English Comments
Peel Strength 0.03287 kN/m
0.1875 pli
Steel, 180° Peel, 72 hr dwell, Backside; ASTM D3330
0.5478 kN/m
3.125 pli
Steel, 180° Peel, 72 hr dwell, Faceside; ASTM D3330
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 70.0 °C
158 °F
Processing Properties Metric English Comments
Shelf Life 24.0 Month
24.0 Month
Descriptive Properties Value Comments
Adhesive Carrier Clear Polyester
Adhesive Type Backside
Faceside
Appearance Translucent
Liner 70# White Polycoated Kraft