Hexcel® HexPly® F522 Epoxy Resin, 7781 Glass Fabric

Category Polymer , Thermoset , Epoxy , Epoxy/Glass SMC
Manufacturer Hexcel
Trade Name HexPly®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Hexcel® HexPly® F522 Epoxy Resin, 7781 Glass Fabric.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Hexcel designation: 7781-38"-F522; Fiber: 75-1/0Information provided by HexCel
Mechanical Properties Metric English Comments
Tensile Strength, Yield 379 MPa

@Temperature 71.0 °C
55000 psi

@Temperature 160 °F
Dry
448 MPa

@Temperature 24.0 °C
65000 psi

@Temperature 75.2 °F
Dry
Tensile Modulus 22.0 GPa

@Temperature 71.0 °C
3190 ksi

@Temperature 160 °F
Dry
22.4 GPa

@Temperature 24.0 °C
3250 ksi

@Temperature 75.2 °F
Dry
Flexural Yield Strength 586 MPa

@Temperature 24.0 °C
85000 psi

@Temperature 75.2 °F
Dry
Compressive Yield Strength 276 MPa

@Temperature 71.0 °C
40000 psi

@Temperature 160 °F
Wet (14 ± 1/2 days of water immersion at 160 ± 5°F (71 ± 3°C)
483 MPa

@Temperature 24.0 °C
70100 psi

@Temperature 75.2 °F
Dry
Shear Strength 58.6 MPa

@Temperature 24.0 °C
8500 psi

@Temperature 75.2 °F
Short Beam, Dry
Descriptive Properties Value Comments
Fiber Volume (%) 0.025