Material Notes:
This adhesive meets the requirements of most long-term applications. It offers temperature resistance to 400°F (204°C). Peel adhesion values are excellent on most membrane switch substrate materials. It features exceptional shear strength and adhesion to high surface energy (HSE) plastics and metal surfaces.Single side spacers aid in the construction of membrane switch circuiry, i.e. to protect leads, hold domes in place, or build spacersInformation provided by 3M
Physical Properties Metric English Comments
Thickness 50.8 microns
2.00 mil
Adhesive
76.2 microns
3.00 mil
Polyester
Mechanical Properties Metric English Comments
Peel Strength 0.153 kN/m
0.875 pli
90° Peel, PET/Polycarbonate, 72 hrs at 70°C; ASTM D3330
0.36156 kN/m
2.0625 pli
90° Peel, PET/Stainless Steel, Initial (20 mins); ASTM D3330
0.4602 kN/m
2.625 pli
90° Peel, PET/Polycarbonate, Initial (20 mins); ASTM D3330
0.482 kN/m
2.75 pli
90° Peel, PET/PET, Initial (20 mins); ASTM D3330
0.526 kN/m
3.00 pli
90° Peel, PET/Aluminum, Initial (20 mins); ASTM D3330
0.69024 kN/m
3.9375 pli
90° Peel, PET/PET, 72 hrs at RT; ASTM D3330
0.701 kN/m
4.00 pli
90° Peel, PET/Polycarbonate, 72 hrs at RT; ASTM D3330
0.79981 kN/m
4.5625 pli
90° Peel, PET/Stainless Steel, 72 hrs at RT; ASTM D3330
0.920 kN/m
5.25 pli
90° Peel, PET/Aluminum, 72 hrs at RT; ASTM D3330
1.62 kN/m
9.25 pli
90° Peel, PET/Stainless Steel, 72 hrs at 70°C; ASTM D3330
2.0379 kN/m
11.625 pli
90° Peel, PET/Aluminum, 72 hrs at 70°C0; ASTM D3330
2.136 kN/m
12.19 pli
90° Peel, PET/PET, 72 hrs at 70°C; ASTM D3330
Thermal Properties Metric English Comments
CTE, linear 3.90 µm/m-°C

@Temperature 27.0 - 175 °C
2.17 µin/in-°F

@Temperature 80.6 - 347 °F
ASTM D696
Electrical Properties Metric English Comments
Volume Resistivity 3.30e+15 ohm-cm
3.30e+15 ohm-cm
ASTM D257
Surface Resistance >= 5.60e+16 ohm
>= 5.60e+16 ohm
ASTM D257
Insulation Resistance 9.40e+12 ohm
9.40e+12 ohm
100VDC, 60 sec; Mil-I-46058C
Dielectric Constant 3.03
3.03
ASTM D150
Dielectric Strength 66.9 kV/mm
1700 kV/in
ASTM D149
Dissipation Factor 0.0090
0.0090
ASTM D150
Descriptive Properties Value Comments
Adhesive Type 200MP
Liner 94# PCK 7.0