Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

3M 7840 Laser Toner Printable Polyester Label Material

Category Polymer , Adhesive
Manufacturer 3M
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M 7840 Laser Toner Printable Polyester Label Material.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
3M™ Laser Toner Printable Polyester Label Materials 7840 and 7840TL are matte radiant white polyester label stocks that offer . These label products utilize 3M™ Adhesive 310 which is a firm adhesive which resists oozing and provides high strength on a variety of surfaces including high surface energy (HSE) plastics and metals.Information provided by 3M
Physical Properties Metric English Comments
Thickness 20.3 microns
0.800 mil
Adhesive
58.4 microns
2.30 mil
Facestock, Matte radiant white polyester
81.3 microns
3.20 mil
Liner
Mechanical Properties Metric English Comments
Peel Strength 0.05478 kN/m
0.3125 pli
LD Polyethylene, 180° Peel, Conditioned for 3 days at 49°C; ASTM D3330
0.0877 kN/m
0.500 pli
LD Polyethylene, 90° Peel, Conditioned for 3 days at 49°C; ASTM D3330
0.131 kN/m
0.750 pli
LD Polyethylene, 90° Peel, Initial, 10 min dwell at RT; ASTM D3330
0.175 kN/m
1.00 pli
Polypropylene, 90° Peel, Initial, 10 min dwell at RT; ASTM D3330
0.175 kN/m
1.00 pli
HD Polyethylene, 90° Peel, Initial, 10 min dwell at RT; ASTM D3330
0.1972 kN/m
1.125 pli
Polypropylene, 180° Peel, Initial, 10 min dwell at RT; ASTM D3330
0.1972 kN/m
1.125 pli
Polypropylene, 180° Peel, Conditioned for 3 days at RT; ASTM D3330
0.219 kN/m
1.25 pli
LD Polyethylene, 180° Peel, Initial, 10 min dwell at RT; ASTM D3330
0.219 kN/m
1.25 pli
HD Polyethylene, 90° Peel, Conditioned for 3 days at RT; ASTM D3330
0.219 kN/m
1.25 pli
HD Polyethylene, 90° Peel, Conditioned for 3 days at 49°C; ASTM D3330
0.219 kN/m
1.25 pli
LD Polyethylene, 180° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330
0.2410 kN/m
1.375 pli
LD Polyethylene, 90° Peel, Conditioned for 3 days at RT; ASTM D3330
0.263 kN/m
1.50 pli
HD Polyethylene, 180° Peel, Initial, 10 min dwell at RT; ASTM D3330
0.263 kN/m
1.50 pli
Polypropylene, 90° Peel, Conditioned for 3 days at RT; ASTM D3330
0.263 kN/m
1.50 pli
LD Polyethylene, 90° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330
0.29582 kN/m
1.6875 pli
Polypropylene, 90° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330
0.29582 kN/m
1.6875 pli
HD Polyethylene, 90° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330
0.3287 kN/m
1.875 pli
HD Polyethylene, 180° Peel, Conditioned for 3 days at 49°C; ASTM D3330
0.3287 kN/m
1.875 pli
Polypropylene, 90° Peel, Conditioned for 3 days at 49°C; ASTM D3330
0.351 kN/m
2.00 pli
LD Polyethylene, 180° Peel, Conditioned for 3 days at RT; ASTM D3330
0.351 kN/m
2.00 pli
Polycarbonate 90° Peel, Conditioned for 3 days at 49°C; ASTM D3330
0.351 kN/m
2.00 pli
Glass, 90° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330
0.36156 kN/m
2.0625 pli
HD Polyethylene, 180° Peel, Conditioned for 3 days at RT; ASTM D3330
0.3725 kN/m
2.125 pli
Glass, 90° Peel, Initial, 10 min dwell at RT; ASTM D3330
0.38347 kN/m
2.1875 pli
Stainless Steel, 90° Peel, Initial, 10 min dwell at RT; ASTM D3330
0.38347 kN/m
2.1875 pli
Polypropylene, 180° Peel, Conditioned for 3 days at 49°C; ASTM D3330
0.38347 kN/m
2.1875 pli
HD Polyethylene, 180° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330
0.40538 kN/m
2.3125 pli
Polycarbonate 90° Peel, Initial, 10 min dwell at RT; ASTM D3330
0.4163 kN/m
2.375 pli
Polypropylene, 180° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330
0.438 kN/m
2.50 pli
Polycarbonate 90° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330
0.44921 kN/m
2.5625 pli
Stainless Steel, 90° Peel, Conditioned for 3 days at RT; ASTM D3330
0.44921 kN/m
2.5625 pli
Polycarbonate 180° Peel, Conditioned for 3 days at 49°C; ASTM D3330
0.4602 kN/m
2.625 pli
Glass, 90° Peel, Conditioned for 3 days at 49°C; ASTM D3330
0.47112 kN/m
2.6875 pli
Stainless Steel, 180° Peel, Initial, 10 min dwell at RT; ASTM D3330
0.47112 kN/m
2.6875 pli
Polycarbonate 90° Peel, Conditioned for 3 days at RT; ASTM D3330
0.5040 kN/m
2.875 pli
Stainless Steel, 90° Peel, Conditioned for 3 days at 49°C; ASTM D3330
0.5040 kN/m
2.875 pli
Stainless Steel, 90° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330
0.51494 kN/m
2.9375 pli
Polycarbonate 180° Peel, Initial, 10 min dwell at RT; ASTM D3330
0.51494 kN/m
2.9375 pli
Glass, 90° Peel, Conditioned for 3 days at RT; ASTM D3330
0.55877 kN/m
3.1875 pli
Stainless Steel, 180° Peel, Conditioned for 3 days at RT; ASTM D3330
0.570 kN/m
3.25 pli
Glass, 180° Peel, Initial, 10 min dwell at RT; ASTM D3330
0.570 kN/m
3.25 pli
Polycarbonate 180° Peel, Conditioned for 3 days at RT; ASTM D3330
0.657 kN/m
3.75 pli
Stainless Steel, 180° Peel, Conditioned for 3 days at 49°C; ASTM D3330
0.6793 kN/m
3.875 pli
Polycarbonate 180° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330
0.7231 kN/m
4.125 pli
Glass, 180° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330
0.745 kN/m
4.25 pli
Glass, 180° Peel, Conditioned for 3 days at RT; ASTM D3330
0.745 kN/m
4.25 pli
Glass, 180° Peel, Conditioned for 3 days at 49°C; ASTM D3330
0.8108 kN/m
4.625 pli
Stainless Steel, 180° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330
Processing Properties Metric English Comments
Shelf Life 12.0 Month
12.0 Month
Descriptive Properties Value Comments
Adhesive Type #310 Acrylic
Liner 55# Densified kraft