AlphaGary Dural 725C CLEAR 0003 Full Rigid Polyvinyl Chloride Compound |
PVC, Rigid Grade |
Dural
|
AlphaGary Garaflex™ E 4362 A1 LCF Vinyl Thermoplastic Elastomer |
PVC, Wire and Cable Grade |
Garaflex™ E
|
AlphaGary Garaflex™ E 4762 A1 LCF Vinyl Thermoplastic Elastomer |
PVC, Wire and Cable Grade |
Garaflex™ E
|
AlphaGary Garaflex™ E 4762-A5 LCF Vinyl Thermoplastic Elastomer |
PVC, Wire and Cable Grade |
Garaflex™ E
|
AlphaGary Garaflex™ E 4777-A6 LCF Vinyl Thermoplastic Elastomer |
PVC, Wire and Cable Grade |
Garaflex™ E
|
AlphaGary Garaflex™ E 50-10 B Vinyl Thermoplastic Elastomer |
PVC, Wire and Cable Grade |
Garaflex™ E
|
AlphaGary Garaflex™ E 89-086 C3 NF LCF-R Vinyl Thermoplastic Elastomer |
PVC, Wire and Cable Grade |
Garaflex™ E
|
AlphaGary Garaflex™ E X 00-207F UV-FG LCF Vinyl Thermoplastic Elastomer |
PVC, Wire and Cable Grade |
Garaflex™ E
|
AlphaGary Garaflex™ E X 05-384-G LCF Vinyl Thermoplastic Elastomer |
PVC, Wire and Cable Grade |
Garaflex™ E
|
AlphaGary Garaflex™ X 05-309 A1 Vinyl Thermoplastic Elastomer |
Vinyl (PVC) |
Garaflex™
|
AlphaGary Garaflex™ X 95-759 B-1 Vinyl Thermoplastic Elastomer |
Vinyl (PVC) |
Garaflex™
|
AlphaGary Garaflex™ X 97-234 D Vinyl Thermoplastic Elastomer |
Vinyl (PVC) |
Garaflex™
|
AlphaGary Garathane™ GT 5080 A Polyurethane based compound |
Polyurethane, TP |
Garathane™
|
AlphaGary GW 3040 LCF Flame Retardant Polyvinyl Chloride |
PVC, Wire and Cable Grade |
GW
|
AlphaGary PVC 2212/7-118 CLEAR 0003 Polyvinyl Chloride Thermoplastic |
PVC, Transparent |
PVC
|
AlphaGary PVC 2212/S-110 CLEAR 0003 Polyvinyl Chloride Thermoplastic |
PVC, Transparent |
PVC
|
AlphaGary PVC 2212-100 CLEAR 0003 Polyvinyl Chloride Thermoplastic |
PVC, Transparent |
PVC
|
AlphaGary PVC 2215/3X-55 Black 1000 Polyvinyl Chloride Thermoplastic |
PVC, Molded |
PVC
|
AlphaGary PVC 2222C-75 CLEAR 0003 Polyvinyl Chloride Thermoplastic |
PVC, Transparent |
PVC
|
AlphaGary PVC 2222NK-70 CLEAR 0217 Polyvinyl Chloride Thermoplastic |
PVC, Transparent |
PVC
|
AlphaGary PVC 2222RX/1-74 CLEAR 0001 Polyvinyl Chloride Thermoplastic |
PVC, Transparent |
PVC
|
AlphaGary PVC 2228GBF-75 CLEAR 000X Polyvinyl Chloride Thermoplastic |
PVC, Transparent |
PVC
|
AlphaGary PVC 3019-40/45 CLEAR 0003 Polyvinyl Chloride Thermoplastic |
PVC, Transparent |
PVC
|
AlphaGary PVC 3032-95 CLEAR 0003 Polyvinyl Chloride Thermoplastic |
PVC, Transparent |
PVC
|
AlphaGary PVC 7762 Polyvinyl Chloride Thermoplastic |
PVC, Molded |
PVC
|
AlphaGary PVC AG K580A Q2 Polyvinyl Chloride Thermoplastic |
PVC, Flexible Grade |
PVC
|
AlphaGary PVC FM1R Polyvinyl Chloride Thermoplastic |
PVC, Extruded |
PVC
|
AlphaGary PVC GEX 03-033 F Natural Polyvinyl Chloride Thermoplastic |
PVC, Extruded |
PVC
|
AlphaGary PVC GM 8015-M Natural LCF Polyvinyl Chloride Thermoplastic |
PVC, Molded |
PVC
|
AlphaGary PVC GM 8015-O Natural LCF Polyvinyl Chloride Thermoplastic |
PVC, Molded |
PVC
|
AlphaGary PVC GM 8017 Natural Polyvinyl Chloride Thermoplastic |
PVC, Molded |
PVC
|
AlphaGary Smokeguard™ LS III 1041 B Low Smoke Polyvinyl Chloride |
PVC, Wire and Cable Grade |
Smokeguard™ LS
|
AlphaGary Smokeguard™ LS III 1093 Low Smoke Polyvinyl Chloride |
PVC, Wire and Cable Grade |
Smokeguard™ LS
|
AlphaGary Smokeguard™ LS III 1096 Low Smoke Polyvinyl Chloride |
PVC, Wire and Cable Grade |
Smokeguard™ LS
|
AlphaGary Smokeguard™ LS IV 1320 Low Smoke Polyvinyl Chloride |
PVC, Wire and Cable Grade |
Smokeguard™ LS
|
AlphaGary Smokeguard™ LS V 1116 Low Smoke Polyvinyl Chloride |
PVC, Wire and Cable Grade |
Smokeguard™ LS
|
AlphaGary Smokeguard™ LS V 1118 Low Smoke Polyvinyl Chloride |
PVC, Wire and Cable Grade |
Smokeguard™ LS
|
AlphaGary SuperKleen SK/2223-80 CLEAR 0002 Flexible Polyvinyl Chloride Compound |
PVC, Flexible Grade |
SuperKleen
|
AlphaGary SuperKleen SK/2223C-70 CLEAR 0001 DB Flexible Polyvinyl Chloride Compound |
PVC, Flexible Grade |
SuperKleen
|
AlphaGary SuperKleen SK/3003-85 CLEAR 0003 Flexible Polyvinyl Chloride Compound |
PVC, Flexible Grade |
SuperKleen
|
AlphaGary Vythene™ VYT/13E-55 CLEAR TL 0025 Polyurethane / Polyvinyl Chloride Compound |
Polyurethane, TP |
Vythene™
|
AlphaGary Garaflex™ 131 T Vinyl Thermoplastic Elastomer |
Vinyl (PVC) |
Garaflex™
|
AlphaGary Garaflex™ E 4780-A5 LCF Vinyl Thermoplastic Elastomer |
PVC, Wire and Cable Grade |
Garaflex™ E
|
AlphaGary Garaflex™ E 4832 Natural UV LCF Vinyl Thermoplastic Elastomer |
PVC, Wire and Cable Grade |
Garaflex™ E
|
AlphaGary GW 2038 VW1 LCF Flame Retardant Polyvinyl Chloride |
PVC, Wire and Cable Grade |
GW
|
AlphaGary GW 2052 SPECIAL LCF Flame Retardant Polyvinyl Chloride |
PVC, Wire and Cable Grade |
GW
|
AlphaGary GW 2105FR-80 CLEAR 0002 Flame Retardant Polyvinyl Chloride |
PVC, Wire and Cable Grade |
GW
|
AlphaGary GW 2280 M VW1 LCF Flame Retardant Polyvinyl Chloride |
PVC, Wire and Cable Grade |
GW
|
AlphaGary GW 2403-1 VW1 105-LCF Flame Retardant Polyvinyl Chloride |
PVC, Wire and Cable Grade |
GW
|
AlphaGary GW 2403-1 VW1 75 LCF Flame Retardant Polyvinyl Chloride |
PVC, Wire and Cable Grade |
GW
|
AlphaGary GW 2409 VW1 50 LCF Flame Retardant Polyvinyl Chloride |
PVC, Wire and Cable Grade |
GW
|
AlphaGary GW 2450-VW1 03 LCF Flame Retardant Polyvinyl Chloride |
PVC, Wire and Cable Grade |
GW
|
AlphaGary GW 2462 H VW1 LCF Flame Retardant Polyvinyl Chloride |
PVC, Wire and Cable Grade |
GW
|
AlphaGary GW 2463 H VW1 LCF Flame Retardant Polyvinyl Chloride |
PVC, Wire and Cable Grade |
GW
|
AlphaGary GW 3003 LCF Q Flame Retardant Polyvinyl Chloride |
PVC, Wire and Cable Grade |
GW
|
AlphaGary GW 3025 VW1 LCF Flame Retardant Polyvinyl Chloride |
PVC, Wire and Cable Grade |
GW
|
AlphaGary GW 3026 A LCF Flame Retardant Polyvinyl Chloride |
PVC, Wire and Cable Grade |
GW
|
AlphaGary GW 3026 LCF Flame Retardant Polyvinyl Chloride |
PVC, Wire and Cable Grade |
GW
|
AlphaGary GW 3028 LCF Flame Retardant Polyvinyl Chloride |
PVC, Wire and Cable Grade |
GW
|
AlphaGary GW 3035-VW1 LCF Flame Retardant Polyvinyl Chloride |
PVC, Wire and Cable Grade |
GW
|
AlphaGary GW 3040 LT LCF Flame Retardant Polyvinyl Chloride |
PVC, Wire and Cable Grade |
GW
|
AlphaGary GW 3042 LCF Flame Retardant Polyvinyl Chloride |
PVC, Wire and Cable Grade |
GW
|
AlphaGary PVC 2212C2B/H-118 CLEAR 0003 Polyvinyl Chloride Thermoplastic |
PVC, Transparent |
PVC
|
AlphaGary PVC 2212RSM-100 CLEAR 000X Polyvinyl Chloride Thermoplastic |
PVC, Transparent |
PVC
|
AlphaGary PVC 2222R-90 CLEAR 000X Polyvinyl Chloride Thermoplastic |
PVC, Transparent |
PVC
|
AlphaGary PVC 2228C/FS-65S WHITE 4001 Polyvinyl Chloride Thermoplastic |
PVC, Extruded |
PVC
|
AlphaGary PVC 2232A/R-80S CLEAR 0217 Polyvinyl Chloride Thermoplastic |
PVC, Transparent |
PVC
|
AlphaGary PVC 2232RSM-100 CLEAR 000X Polyvinyl Chloride Thermoplastic |
PVC, Transparent |
PVC
|
AlphaGary PVC 2233AXLT-68 CLEAR 0198 Polyvinyl Chloride Thermoplastic |
PVC, Transparent |
PVC
|
AlphaGary PVC 2235L-75 CLEAR 030X Polyvinyl Chloride Thermoplastic |
PVC, Transparent |
PVC
|
AlphaGary PVC 2235LM-95 CLEAR 000X Polyvinyl Chloride Thermoplastic |
PVC, Transparent |
PVC
|
AlphaGary PVC 2235RSM-100 CLEAR 000X Polyvinyl Chloride Thermoplastic |
PVC, Transparent |
PVC
|
AlphaGary PVC 3006-90 CLEAR 0217 Polyvinyl Chloride Thermoplastic |
PVC, Transparent |
PVC
|
AlphaGary PVC 3006R-90 CLEAR 000X Polyvinyl Chloride Thermoplastic |
PVC, Transparent |
PVC
|
AlphaGary PVC GSX 05-309 A2 UV Polyvinyl Chloride Thermoplastic |
PVC, Flexible Grade |
PVC
|
AlphaGary Smokeguard™ LS III 1021 UV FG Low Smoke Polyvinyl Chloride |
PVC, Wire and Cable Grade |
Smokeguard™ LS
|
AlphaGary Smokeguard™ LS III 1022 Low Smoke Polyvinyl Chloride |
PVC, Wire and Cable Grade |
Smokeguard™ LS
|
AlphaGary Smokeguard™ LS III 1028 Low Smoke Polyvinyl Chloride |
PVC, Wire and Cable Grade |
Smokeguard™ LS
|
AlphaGary Smokeguard™ LS III 1041 Low Smoke Polyvinyl Chloride |
PVC, Wire and Cable Grade |
Smokeguard™ LS
|
AlphaGary Smokeguard™ LS III 1042 B Low Smoke Polyvinyl Chloride |
PVC, Wire and Cable Grade |
Smokeguard™ LS
|
AlphaGary Smokeguard™ LS III 1056 Low Smoke Polyvinyl Chloride |
PVC, Wire and Cable Grade |
Smokeguard™ LS
|
AlphaGary Smokeguard™ LS III 1057 Low Smoke Polyvinyl Chloride |
PVC, Wire and Cable Grade |
Smokeguard™ LS
|
AlphaGary Smokeguard™ LS III 1071 A Low Smoke Polyvinyl Chloride |
PVC, Wire and Cable Grade |
Smokeguard™ LS
|
AlphaGary Smokeguard™ LS III 1080 C Low Smoke Polyvinyl Chloride |
PVC, Wire and Cable Grade |
Smokeguard™ LS
|
AlphaGary Smokeguard™ LS III 1091 A1 Low Smoke Polyvinyl Chloride |
PVC, Wire and Cable Grade |
Smokeguard™ LS
|
AlphaGary Vythene™ VYT/11X-50 RV1 CLEAR TL 0002 Polyurethane / Polyvinyl Chloride Compound |
Polyurethane, TP |
Vythene™
|
AlphaGary Dural 202/3 CLEAR 0003 Full Rigid Polyvinyl Chloride Compound |
PVC, Rigid Grade |
Dural
|
AlphaGary Dural 205JB CLEAR 0003 Full Rigid Polyvinyl Chloride Compound |
PVC, Rigid Grade |
Dural
|
AlphaGary GW 2326 A VW1 LCF Flame Retardant Polyvinyl Chloride |
PVC, Wire and Cable Grade |
GW
|
AlphaGary GW 2403-1 VW1 LCF Flame Retardant Polyvinyl Chloride |
PVC, Wire and Cable Grade |
GW
|
AlphaGary GW 3010 LCF P Flame Retardant Polyvinyl Chloride |
PVC, Wire and Cable Grade |
GW
|
AlphaGary PVC 2212RHT/1-118 CLEAR 080X Polyvinyl Chloride Thermoplastic |
PVC, Transparent |
PVC
|
AlphaGary PVC 3016GBF-70S CLEAR 000X Polyvinyl Chloride Thermoplastic |
PVC, Transparent |
PVC
|
AlphaGary PVC 7731 Polyvinyl Chloride Thermoplastic |
PVC, Molded |
PVC
|
AlphaGary PVC 7732 Polyvinyl Chloride Thermoplastic |
PVC, Extruded |
PVC
|
AlphaGary PVC 7761 Polyvinyl Chloride Thermoplastic |
PVC, Extruded |
PVC
|
AlphaGary PVC AG K580D N14A Polyvinyl Chloride Thermoplastic |
PVC, Flexible Grade |
PVC
|
AlphaGary PVC FMPP - Clear, Various Colors Polyvinyl Chloride Thermoplastic |
PVC, Extruded |
PVC
|
AlphaGary PVC GEX 03-040 F Polyvinyl Chloride Thermoplastic |
PVC, Extruded |
PVC
|
AlphaGary PVC GM 5055 Natural Polyvinyl Chloride Thermoplastic |
PVC, Molded |
PVC
|