Category | Polymer , Thermoplastic , Vinyl (PVC) , PVC, Wire and Cable Grade |
Manufacturer | AlphaGary |
Trade Name | GW |
Port | Shanghai port,China |
Trade Terms | FOB, CFR, CIF |
Payment Terms | L/C, T/T, Western Union |
Download PDF | AlphaGary GW 2105FR-80 CLEAR 0002 Flame Retardant Polyvinyl Chloride.pdf ![]() |
Price | EMAIL US sales@lookpolymers.com |
Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 22.1 MPa | 3200 psi | |
Elongation at Break | 325 % | 325 % | ASTM D412 |
Thermal Properties | Metric | English | Comments |
---|---|---|---|
Brittleness Temperature | -25.0 °C | -13.0 °F |
Optical Properties | Metric | English | Comments |
---|---|---|---|
Transmission, Visible | 90 % | 90 % | clear; thickness not quantified |