Category | Polymer , Thermoplastic , Vinyl (PVC) , PVC, Wire and Cable Grade |
Manufacturer | AlphaGary |
Trade Name | GW |
Port | Shanghai port,China |
Trade Terms | FOB, CFR, CIF |
Payment Terms | L/C, T/T, Western Union |
Download PDF | AlphaGary GW 2326 A VW1 LCF Flame Retardant Polyvinyl Chloride.pdf ![]() |
Price | EMAIL US sales@lookpolymers.com |
Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 17.9 MPa | 2600 psi | |
Elongation at Break | 330 % | 330 % | ASTM D412 |
Thermal Properties | Metric | English | Comments |
---|---|---|---|
Brittleness Temperature | -48.0 °C | -54.4 °F | |
Oxygen Index | 28 % | 28 % |