AlphaGary PVC 7732 Polyvinyl Chloride Thermoplastic

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Extruded
Manufacturer AlphaGary
Trade Name PVC
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF AlphaGary PVC 7732 Polyvinyl Chloride Thermoplastic.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Automotive Extrusion
Physical Properties Metric English Comments
Specific Gravity 1.35 g/cc
1.35 g/cc
Mechanical Properties Metric English Comments
Hardness, Shore A 97
97
Tensile Strength 13.1 MPa
1900 psi
Elongation at Break 220 %
220 %