Category | Polymer , Thermoplastic , Vinyl (PVC) , PVC, Flexible Grade |
Manufacturer | AlphaGary |
Trade Name | PVC |
Port | Ningbo port,China |
Trade Terms | FOB, CFR, CIF |
Payment Terms | L/C, T/T, Western Union |
Download PDF | AlphaGary PVC AG K580D N14A Polyvinyl Chloride Thermoplastic.pdf ![]() |
Price | EMAIL US sales@lookpolymers.com |
Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 1.24 g/cc | 1.24 g/cc |
Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Hardness, Shore A | 60 | 60 | |
Tensile Strength | 7.58 MPa | 1100 psi | |
Elongation at Break | 375 % | 375 % |