Category | Polymer , Thermoplastic , Elastomer, TPE , Vinyl (PVC) , PVC, Wire and Cable Grade |
Manufacturer | AlphaGary |
Trade Name | Garaflex™ E |
Port | Ningbo port,China |
Trade Terms | FOB, CFR, CIF |
Payment Terms | L/C, T/T, Western Union |
Download PDF | AlphaGary Garaflex™ E X 05-384-G LCF Vinyl Thermoplastic Elastomer.pdf ![]() |
Price | EMAIL US sales@lookpolymers.com |
Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Hardness, Shore A | 70 - 80 | 70 - 80 | |
Tensile Strength | 9.31 MPa | 1350 psi | |
Elongation at Break | 280 % | 280 % | ASTM D412 |
Thermal Properties | Metric | English | Comments |
---|---|---|---|
Brittleness Temperature | -28.0 °C | -18.4 °F |