Electrical Properties | Metric | English | Comments |
---|---|---|---|
Comparative Tracking Index | 600 V @Thickness 3.20 mm |
600 V @Thickness 0.126 in |
Sol. A; IEC 112, UL 746A |
Nilit Nilamid A G5 FR PH2 25% Glass Fiber Reinforced, Flame Retardant PA66 (with Red Phosphorous) Description: Nilamid A G5 FR PH2 combines flame retardancy with outstanding mechanical performance. This product has a complete yellow card, with RTI and CTI listings. The formulation has been optim.. |
|||
Comparative Tracking Index | 600 V @Thickness 3.20 mm |
600 V @Thickness 0.126 in |
Sol. B; IEC 112, UL 746A |
Nilit Nilamid A G5 FR PH2 25% Glass Fiber Reinforced, Flame Retardant PA66 (with Red Phosphorous) Description: Nilamid A G5 FR PH2 combines flame retardancy with outstanding mechanical performance. This product has a complete yellow card, with RTI and CTI listings. The formulation has been optim.. |
|||
Comparative Tracking Index | >= 600 V @Thickness 3.20 mm |
>= 600 V @Thickness 0.126 in |
Sol. A; IEC 112, UL 746A |
Nilit Nilamid A H2 FR HF2 Unfilled, Flame Retardant PA66/6 Co-Polymer Description: Nilamid A H2 FR HF2 is an unfilled, flame retardant NYLON 66/6 co-polymer that does not contain halogen or red phosphorous. This product combines excellent flow characteristics and extr.. |
|||
Comparative Tracking Index | >= 600 V @Thickness 3.20 mm |
>= 600 V @Thickness 0.126 in |
Sol. B; IEC 112, UL 746A |
Nilit Nilamid A H2 FR HF2 Unfilled, Flame Retardant PA66/6 Co-Polymer Description: Nilamid A H2 FR HF2 is an unfilled, flame retardant NYLON 66/6 co-polymer that does not contain halogen or red phosphorous. This product combines excellent flow characteristics and extr.. |
|||
Comparative Tracking Index | 600 V @Thickness 3.20 mm |
600 V @Thickness 0.126 in |
Sol. A; IEC 112, UL 746A |
Nilit Nilamid A3 H G3 15% Glass Reinforced PA66 Description: Nilamid A3 H G3 is a general purpose, 15% glass fiber reinforced NYLON 66. This product combines good overall mechanical performance and impact strength with ease of processing.Key char.. |
|||
Comparative Tracking Index | 600 V @Thickness 3.20 mm |
600 V @Thickness 0.126 in |
Sol. A; IEC 112, UL 746A |
Nilit Nilamid B3 H ZC Unfilled, Low Temperature Impact Resistant PA6 Description: Nilamid B3 H ZC has outstanding impact performance, even at minus temperatures. It is widely used for components subjected to high shock loads. Applications include bicycle components, .. |
|||
Comparative Tracking Index | 600 V @Thickness 3.20 mm |
600 V @Thickness 0.126 in |
Sol. A; IEC 112, UL 746A |
Nilit Nilamid B3N Unfilled, Nucleated PA6 Description: Nilamid B3N is an unfilled, nucleated NYLON 6. It is fast cycling, and combines ease of processing with good overall mechanical characteristics.Key characteristics: Fast cyclingEasy pro.. |
|||
Comparative Tracking Index | 600 V @Thickness 3.20 mm |
600 V @Thickness 0.126 in |
Sol. B; IEC 112, UL 746A |
Nilit Nilamid B3N Unfilled, Nucleated PA6 Description: Nilamid B3N is an unfilled, nucleated NYLON 6. It is fast cycling, and combines ease of processing with good overall mechanical characteristics.Key characteristics: Fast cyclingEasy pro.. |
|||
Comparative Tracking Index | 600 V @Thickness 3.20 mm |
600 V @Thickness 0.126 in |
Sol. A; IEC 112, UL 746A |
Nilit Nilitop BT N Unfilled, Nucleated PBT Description: Nilitop BT N is an unfilled, nucleated PBT that has excellent cycle times.Key characteristics: Good overall mechanical performanceLow moisture absorptionExcellent UV resistanceExcellent.. |
|||
Comparative Tracking Index | 600 V @Temperature 23.0 °C |
600 V @Temperature 73.4 °F |
IEC 60112 |
DuPont Performance Polymers Crastin® S600F20 NC010 PBT
(Unverified Data**) Crastin® S600F20 NC010 is an unreinforced, lubricated, medium viscosity polybutylene terephthalate resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Comparative Tracking Index | 600 V @Temperature 23.0 °C |
600 V @Temperature 73.4 °F |
IEC 60112 |
DuPont Performance Polymers Crastin® S620F20 BK851 PBT
(Unverified Data**) Crastin® S620F20 BK851 is an unreinforced, nucleated, lubricated, medium viscosity, black polybutylene terephthalate resin for fast injection molding.Information provided by DuPont Performance Poly.. |
|||
Comparative Tracking Index | 600 V @Thickness 3.20 mm |
600 V @Thickness 0.126 in |
Sol. B; IEC 112, UL 746A |
Nilit Nilamid A3 H ZB High Impact PA66 Description: Nilamid A3 H ZB is high impact NYLON 66. The product maintains excellent impact properties, even at minus temperatures, whilst maintaining mechanical characteristics. Application areas .. |
|||
Comparative Tracking Index | 600 V @Thickness 3.20 mm |
600 V @Thickness 0.126 in |
Sol. A; IEC 112, UL 746A |
Nilit Nilamid A3 H ZC High Impact PA66 Description: Nilamid A3 H ZC has outstanding impact performance, even at minus temperatures. It is widely used for components subjected to high shock loads. Applications include bicycle components, .. |
|||
Comparative Tracking Index | 600 V @Thickness 3.20 mm |
600 V @Thickness 0.126 in |
Sol. B; IEC 112, UL 746A |
Nilit Nilamid A3 H ZC High Impact PA66 Description: Nilamid A3 H ZC has outstanding impact performance, even at minus temperatures. It is widely used for components subjected to high shock loads. Applications include bicycle components, .. |
|||
Comparative Tracking Index | 600 V @Thickness 3.20 mm |
600 V @Thickness 0.126 in |
Sol. A; IEC 112, UL 746A |
Nilit Nilamid A3 N H2 Nucleated, Heat Stabilized Nylon 66 Description: Nilamid A3 N H2 is a nucleated, heat stabilized NYLON 66 with excellent flow characteristics and very fast cycle time. It is widely used throughout many industries for mass production a.. |
|||
Comparative Tracking Index | 600 V @Thickness 3.20 mm |
600 V @Thickness 0.126 in |
Sol. A; IEC 112, UL 746A |
Nilit Nilamid B3 H XB Unfilled, Impact Resistant PA6 Description: Nilamid B3 H XB is a high impact NYLON 6. The product has excellent impact properties above 0°C, combined with good maintaining mechanical characteristics. Application areas include au.. |
|||
Comparative Tracking Index | 600 V @Thickness 3.20 mm |
600 V @Thickness 0.126 in |
Sol. A; IEC 112, UL 746A |
Nilit Nilamid B3 H ZA Unfilled, Low Temperature Impact Resistant PA6 Description: Nilamid B3 H ZA is a NYLON 6 with a low level of impact modification, allowing parts to be snap fitted in a dry-as-molded condition. It also has improved impact strength and elongation,.. |
|||
Comparative Tracking Index | >= 600 V @Temperature 23.0 °C |
>= 600 V @Temperature 73.4 °F |
DAM; UL 746A |
DuPont Performance Polymers Zytel® 103HSL BKB080 Nylon 66
(Unverified Data**) Zytel® 103HSL BKB080 is a heat stabilized, lubricated polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Comparative Tracking Index | 600 V @Temperature 23.0 °C |
600 V @Temperature 73.4 °F |
DAM; UL 746A |
DuPont Performance Polymers Zytel® 45HSB NC010 Nylon 66
(Unverified Data**) Zytel® 45HSB NC010 is a high viscosity, heat stabilized polyamide 66 resin for injection molding and extrusion.Information provided by DuPont Performance Polymers |
|||
Comparative Tracking Index | >= 600 V @Thickness 3.00 mm, Temperature 23.0 °C |
>= 600 V @Thickness 0.118 in, Temperature 73.4 °F |
DAM; UL 746A |
DuPont Performance Polymers Zytel® 70G30L NC010 Nylon 66
(Unverified Data**) Zytel® 70G30L NC010 is a 30% glass fiber reinforced polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Comparative Tracking Index | 600 V @Temperature 23.0 °C |
600 V @Temperature 73.4 °F |
50%RH; IEC 60112 |
DuPont Performance Polymers Zytel® E53 NC010 Nylon 66
(Unverified Data**) Zytel® E53 NC010 is a very high viscosity polyamide 66 resin for extrusion.Information provided by DuPont Performance Polymers |
|||
Comparative Tracking Index | 600 V @Temperature 23.0 °C |
600 V @Temperature 73.4 °F |
DAM; IEC 60112 |
DuPont Performance Polymers Zytel® 151 NC010 Nylon 612
(Unverified Data**) Zytel® 151 NC010 is a PA 612 resin.Information provided by DuPont Performance Polymers |
|||
Comparative Tracking Index | >= 600 V @Temperature 23.0 °C |
>= 600 V @Temperature 73.4 °F |
DAM; UL 746A |
DuPont Performance Polymers Zytel® 151 NC010 Nylon 612
(Unverified Data**) Zytel® 151 NC010 is a PA 612 resin.Information provided by DuPont Performance Polymers |
|||
Comparative Tracking Index | 600 V @Temperature 23.0 °C |
600 V @Temperature 73.4 °F |
DAM; IEC 60112 |
DuPont Performance Polymers Zytel® 7301 NC010 Nylon 6
(Unverified Data**) Zytel® 7301 NC010 is a general purpose, unlubricated polyamide 6 resin for extrusion applications.Information provided by DuPont Performance Polymers |
|||
Comparative Tracking Index | 600 V @Temperature 23.0 °C |
600 V @Temperature 73.4 °F |
50%RH; IEC 60112 |
DuPont Performance Polymers Zytel® 7301 NC010 Nylon 6
(Unverified Data**) Zytel® 7301 NC010 is a general purpose, unlubricated polyamide 6 resin for extrusion applications.Information provided by DuPont Performance Polymers |
|||
Comparative Tracking Index | 600 V @Temperature 23.0 °C |
600 V @Temperature 73.4 °F |
DAM; IEC 60112 |
DuPont Performance Polymers Zytel® 77G33HS1L NC010 Nylon 612 Zytel® 77G33HS1L NC010 is a 33% glass fiber reinforced, heat stabilized polyamide 612 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Comparative Tracking Index | 600 V @Temperature 23.0 °C |
600 V @Temperature 73.4 °F |
DAM; IEC 60112 |
DuPont Performance Polymers Zytel® ST801AW BK195 Nylon 66
(Unverified Data**) Zytel® ST801AW BK195 is a Super Tough, weatherable, easy flow and processing friendly, black polyamide 66 resin for injection molding. It offers the best resistance to outdoor exposure.Information.. |
|||
Comparative Tracking Index | 600 V @Temperature 23.0 °C |
600 V @Temperature 73.4 °F |
DAM; UL 746A |
DuPont Performance Polymers Zytel® ST801AW BK195 Nylon 66
(Unverified Data**) Zytel® ST801AW BK195 is a Super Tough, weatherable, easy flow and processing friendly, black polyamide 66 resin for injection molding. It offers the best resistance to outdoor exposure.Information.. |
|||
Comparative Tracking Index | >= 600 V @Thickness 3.00 mm, Temperature 23.0 °C |
>= 600 V @Thickness 0.118 in, Temperature 73.4 °F |
DAM; UL 746A |
DuPont Performance Polymers Zytel® 77G43L NC010 Nylon 612
(Unverified Data**) Zytel® 77G43L NC010 is a 43% glass fiber reinforced polyamide 612 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Comparative Tracking Index | >= 600 V @Thickness 3.00 mm, Temperature 23.0 °C |
>= 600 V @Thickness 0.118 in, Temperature 73.4 °F |
DAM; UL 746A |
DuPont Performance Polymers Zytel® 77G43L NC010 Nylon 612
(Unverified Data**) Zytel® 77G43L NC010 is a 43% glass fiber reinforced polyamide 612 resin for injection molding.Information provided by DuPont Performance Polymers |