Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 1.0 - 1000 ohm-cm | 1.0 - 1000 ohm-cm | ASTM D257 |
PolyOne Stat-Tech™ NN-30CF/000 Black Polyamide 66 (Nylon 66) Stat-Tech™ Electrically Conductive Compounds are specifically engineered to provide anti-static, ESD and RFI/EMI shielding performance for critical electronic equipment applications. These compound.. |
|||
Volume Resistivity | 10 - 1000 ohm-cm | 10 - 1000 ohm-cm | ASTM D257 |
PolyOne Stat-Tech™ X ST6600-0041 ES NHFR Black Polyamide 66 (Nylon 66) Stat-Tech™ Electrically Conductive Compounds are specifically engineered to provide anti-static, ESD and RFI/EMI shielding performance for critical electronic equipment applications. These compound.. |
|||
Volume Resistivity | 10 - 1000 ohm-cm | 10 - 1000 ohm-cm | ASTM D257 |
PolyOne Edgetek® PS-20CF/000 Polybutylene Terephthalate (PBT), Carbon Fiber Reinforced
(discontinued **) Description/Features:Carbon Fiber ReinforcedPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Volume Resistivity | 10 - 1000 ohm-cm | 10 - 1000 ohm-cm | ASTM D257 |
PolyOne Stat-Tech™ ST9620-0020 ES Red Liquid Crystal Polymer + PPS (LCP+PPS) Stat-Tech™ Electrically Conductive Compounds are specifically engineered to provide anti-static, ESD and RFI/EMI shielding performance for critical electronic equipment applications. These compound.. |
|||
Volume Resistivity | 10 - 1000 ohm-cm | 10 - 1000 ohm-cm | ASTM D257 |
PolyOne Edgetek® ATH-20CF/000 Acetal-Homopolymer, Carbon Fiber Reinforced
(discontinued **) Description/Features:Carbon Fiber ReinforcedElectrically ConductivePolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Volume Resistivity | 100 - 1000 ohm-cm | 100 - 1000 ohm-cm | ASTM D257 |
PolyOne Therma-Tech™ SFC-5000 TC Polyphenylene Sulfide (PPS)
(discontinued **) Therma-Tech™ Thermal Management Compounds have been engineered to combine the heat transfer and cooling capabilities of metals with the design freedom, weight reduction and cost advantages of therm.. |
|||
Volume Resistivity | 10 - 1000 ohm-cm | 10 - 1000 ohm-cm | ASTM D257 |
Techmer ES Electrablend® ABS CF20 BK 20% Carbon Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber, 20% Filler by WeightAppearance: BlackInformation provided by TP Composites, Inc. |
|||
Volume Resistivity | 10 - 1000 ohm-cm | 10 - 1000 ohm-cm | ASTM D257 |
Techmer ES Electrablend® ABS CF25 BK 25% Carbon Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber, 25% Filler by WeightAppearance: BlackInformation provided by TP Composites, Inc. |
|||
Volume Resistivity | 1.0 - 1000 ohm-cm | 1.0 - 1000 ohm-cm | ASTM D257 |
Techmer ES Electrablend® PC 04004 FR BK Stainless Steel Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Stainless Steel FiberFeatures: Electromagnetic Shielding (EMI) and Flame RetardantAppearance: BlackTPCI# 9691124Information provided by.. |
|||
Volume Resistivity | 1.0 - 1000 ohm-cm | 1.0 - 1000 ohm-cm | ASTM D257 |
Techmer ES Electrablend® PC 04005 FR BK Stainless Steel Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Stainless Steel FiberFeatures: Electromagnetic Shielding (EMI) and Flame RetardantAppearance: BlackTPCI# 9691124Information provided by.. |
|||
Volume Resistivity | 1.0 - 1000 ohm-cm | 1.0 - 1000 ohm-cm | ASTM D257 |
Techmer ES Electrablend® PC 04007 FR BK Stainless Steel Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Stainless Steel FiberFeatures: Electromagnetic Shielding (EMI) and Flame RetardantAppearance: BlackTPCI# 9691124Information provided by.. |
|||
Volume Resistivity | 1.0 - 1000 ohm-cm | 1.0 - 1000 ohm-cm | ASTM D257 |
Techmer ES Electrablend® PC 05004 FR Stainless Steel Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Stainless Steel FiberFeatures: Electromagnetic Shielding (EMI) and Flame RetardantInformation provided by TP Composites, Inc. |
|||
Volume Resistivity | 1.0 - 1000 ohm-cm | 1.0 - 1000 ohm-cm | ASTM D257 |
Techmer ES Electrablend® PCA 06006 BK Nickel-Coated Carbon Fiber/Stainless Steel Fiber Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Nickel-Coated Carbon Fiber and Stainless Steel FiberFeatures: Electromagnetic Shielding (EMI)Appearance: BlackTPCI# 9691124Information .. |
|||
Volume Resistivity | 10 - 1000 ohm-cm | 10 - 1000 ohm-cm | ASTM D257 |
Techmer ES Electrablend® PPS 05002 Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber ReinforcementFeatures: Electrically ConductiveInformation provided by TP Composites, Inc. |
|||
Volume Resistivity | 10 - 1000 ohm-cm | 10 - 1000 ohm-cm | ASTM D257 |
Techmer ES Electrablend® PPS 06001 Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber ReinforcementFeatures: Electrically ConductiveInformation provided by TP Composites, Inc. |
|||
Volume Resistivity | 1.0 - 1000 ohm-cm | 1.0 - 1000 ohm-cm | ASTM D257 |
Techmer ES Electrablend® ABS 04002 BK 16% Stainless Steel Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Stainless Steel Fiber, 16% Filler by WeightFeatures: Flame Retardant and Electromagnetic Shielding (EMI)Appearance: BlackTPCI# 7965121I.. |
|||
Volume Resistivity | 10 - 1000 ohm-cm | 10 - 1000 ohm-cm | ASTM D257 |
Techmer ES Electrablend® PA6/6 03002 A MB Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement/Unspecified Filler/Reinfor.Additive: Lubricant, Impact Modifier and Heat StabilizerFeatures: Lubricated, Elec.. |
|||
Volume Resistivity | 10 - 1000 ohm-cm | 10 - 1000 ohm-cm | ASTM D257 |
PolyOne Edgetek® AM-30CF/000 Polyphthalamide (PPA), Carbon Fiber Reinforced
(discontinued **) Description/Features:Carbon Fiber ReinforcedPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Volume Resistivity | 10 - 1000 ohm-cm | 10 - 1000 ohm-cm | ASTM D257 |
Techmer ES Electrablend® PC SS15 15% Stainless Steel Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Stainless Steel Fiber, 15% Filler by WeightFeatures: Electromagnetic Shielding (EMI)Information provided by TP Composites, Inc. |