| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Volume Resistivity | 10 - 1000 ohm-cm | 10 - 1000 ohm-cm | ASTM D257 |
| PolyOne Stat-Tech™ NN-40CF/000 NH FRV0 Natural Polyamide 66 (Nylon 66) Stat-Tech™ Electrically Conductive Compounds are specifically engineered to provide anti-static, ESD and RFI/EMI shielding performance for critical electronic equipment applications. These compound.. |
|||
| Volume Resistivity | 10 - 1000 ohm-cm | 10 - 1000 ohm-cm | ASTM D257 |
| PolyOne Stat-Tech™ X ST6600-0041 ES NHFR Black Polyamide 66 (Nylon 66) Stat-Tech™ Electrically Conductive Compounds are specifically engineered to provide anti-static, ESD and RFI/EMI shielding performance for critical electronic equipment applications. These compound.. |
|||
| Volume Resistivity | 10 - 1000 ohm-cm | 10 - 1000 ohm-cm | ASTM D257 |
| PolyOne Edgetek® PS-20CF/000 Polybutylene Terephthalate (PBT), Carbon Fiber Reinforced
(discontinued **) Description/Features:Carbon Fiber ReinforcedPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
| Volume Resistivity | 10 - 1000 ohm-cm | 10 - 1000 ohm-cm | ASTM D257 |
| PolyOne Lubri-Tech™ PI-30CF/15T Polyetherimide (PEI), Carbon Fiber Reinforced, PTFE Lubricated
(discontinued Description/Features:Carbon Fiber ReinforcedPTFE LubricatedPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
| Volume Resistivity | 100 - 1000 ohm-cm | 100 - 1000 ohm-cm | ASTM D257 |
| PolyOne Therma-Tech™ NJC-6000 TC Nylon 12
(discontinued **) Therma-Tech™ Thermal Management Compounds have been engineered to combine the heat transfer and cooling capabilities of metals with the design freedom, weight reduction and cost advantages of therm.. |
|||
| Volume Resistivity | 100 - 1000 ohm-cm | 100 - 1000 ohm-cm | ASTM D257 |
| PolyOne Lubri-Tech™ SF-30CF/13T2S Polyphenylene Sulfide (PPS), Carbon Fiber Reinforced, PTFE/Silicone Lubricated
&n Description/Features:Carbon Fiber ReinforcedPTFE/Silicone LubricatedPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
| Volume Resistivity | 100 - 1000 ohm-cm | 100 - 1000 ohm-cm | ASTM D257 |
| PolyOne Therma-Tech™ SFC-5000 TC Polyphenylene Sulfide (PPS)
(discontinued **) Therma-Tech™ Thermal Management Compounds have been engineered to combine the heat transfer and cooling capabilities of metals with the design freedom, weight reduction and cost advantages of therm.. |
|||
| Volume Resistivity | 1.0 - 1000 ohm-cm | 1.0 - 1000 ohm-cm | ASTM D257 |
| Techmer ES Electrablend® ABS 04001 BK 10% Stainless Steel Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Stainless Steel Fiber, 10% Filler by WeightFeatures: Flame Retardant and Electromagnetic Shielding (EMI)Appearance: BlackTPCI# 7965121I.. |
|||
| Volume Resistivity | 1.0 - 1000 ohm-cm | 1.0 - 1000 ohm-cm | ASTM D257 |
| Techmer ES Electrablend® PC 04004 FR BK Stainless Steel Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Stainless Steel FiberFeatures: Electromagnetic Shielding (EMI) and Flame RetardantAppearance: BlackTPCI# 9691124Information provided by.. |
|||
| Volume Resistivity | 1.0 - 1000 ohm-cm | 1.0 - 1000 ohm-cm | ASTM D257 |
| Techmer ES Electrablend® PC 04005 FR BK Stainless Steel Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Stainless Steel FiberFeatures: Electromagnetic Shielding (EMI) and Flame RetardantAppearance: BlackTPCI# 9691124Information provided by.. |
|||
| Volume Resistivity | 1.0 - 1000 ohm-cm | 1.0 - 1000 ohm-cm | ASTM D257 |
| Techmer ES Electrablend® PC 04006 FR BK Stainless Steel Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Stainless Steel FiberFeatures: Electromagnetic Shielding (EMI) and Flame RetardantAppearance: BlackInformation provided by TP Composite.. |
|||
| Volume Resistivity | 1.0 - 1000 ohm-cm | 1.0 - 1000 ohm-cm | ASTM D257 |
| Techmer ES Electrablend® PEI 04001 MB Stainless Steel Fiber Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Stainless Steel FiberFeatures: Electromagnetic Shielding (EMI)Information provided by TP Composites, Inc. |
|||
| Volume Resistivity | 10 - 1000 ohm-cm | 10 - 1000 ohm-cm | ASTM D257 |
| Techmer ES Electrablend® PPS 05002 Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber ReinforcementFeatures: Electrically ConductiveInformation provided by TP Composites, Inc. |
|||
| Volume Resistivity | 10 - 1000 ohm-cm | 10 - 1000 ohm-cm | ASTM D257 |
| Techmer ES Luriblend® PA6/6 CF20 TS15 BK 20% Carbon Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber, 20% Filler by WeightAdditive: PTFE Lubricant(10%) and Silicone Lubricant Features: Lubricated, Good Wear Resistance and L.. |
|||
| Volume Resistivity | 1.0 - 1000 ohm-cm | 1.0 - 1000 ohm-cm | ASTM D257 |
| Techmer ES Electrablend® ABS 03011 FR BK MB 15% Stainless Steel Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Stainless Steel Fiber, 15% Filler by WeightFeatures: Flame Retardant and Electromagnetic Shielding (EMI)Appearance: BlackTPCI# 7965121I.. |
|||
| Volume Resistivity | 1.0 - 1000 ohm-cm | 1.0 - 1000 ohm-cm | ASTM D257 |
| Techmer ES Electrablend® ABS 04002 BK 16% Stainless Steel Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Stainless Steel Fiber, 16% Filler by WeightFeatures: Flame Retardant and Electromagnetic Shielding (EMI)Appearance: BlackTPCI# 7965121I.. |
|||
| Volume Resistivity | 10 - 1000 ohm-cm | 10 - 1000 ohm-cm | ASTM D257 |
| Techmer ES Electrablend® PA6 CF30 30% Carbon Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber Reinforcement, 30% Filler by WeightFeatures: Conductive Appearance: BlackInformation provided by TP Composites, Inc. |
|||
| Volume Resistivity | 10 - 1000 ohm-cm | 10 - 1000 ohm-cm | ASTM D257 |
| Techmer ES Electrablend® PA6 CF30 TL10 30% Carbon Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber Reinforcement, 30% Filler by WeightAdditive: PTFE Lubricant(10%)Features: Conductive and LubricatedAppearance: BlackInform.. |
|||
| Volume Resistivity | 10 - 1000 ohm-cm | 10 - 1000 ohm-cm | ASTM D257 |
| Techmer ES Electrablend® PA6/6 03002 A MB Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement/Unspecified Filler/Reinfor.Additive: Lubricant, Impact Modifier and Heat StabilizerFeatures: Lubricated, Elec.. |
|||
| Volume Resistivity | 1.0 - 1000 ohm-cm | 1.0 - 1000 ohm-cm | ASTM D257 |
| Techmer ES Electrablend® PA6/6 03002 CF Carbon Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber ReinforcementAdditive: Lubricant, Impact Modifier and Heat StabilizerFeatures: Lubricated, Electrically Conductive, Impact.. |
|||