Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 1.00e+14 - 1.00e+15 ohm-cm | 1.00e+14 - 1.00e+15 ohm-cm | IEC 60093 |
Raschig Group 2557 AMC Polyester Glass fiber reinforced polyester molding compound. Very good mechanical strength, very good electrical properties and dimensional stability, exceptional processability with short cycle time and low .. |
|||
Volume Resistivity | 1.00e+14 - 1.00e+15 ohm-cm | 1.00e+14 - 1.00e+15 ohm-cm | IEC 60093 |
Raschig Group 2568 AMC Glass fiber-reinforced polyester molding compound. Very good mechanical strength, very good electrical properties and dimensional stability, heat resistant up to 500°C for short time - usable for s.. |
|||
Volume Resistivity | 1.00e+14 - 1.00e+15 ohm-cm | 1.00e+14 - 1.00e+15 ohm-cm | IEC 60093 |
Raschig Group 2572 AMC Glass fiber reinforced Polyester molding compound. Very good mechanical strength, very good electrical properties and dimensional stability, good abrasion stability, high flame retardance in combin.. |
|||
Volume Resistivity | 1.00e+14 - 1.00e+15 ohm-cm | 1.00e+14 - 1.00e+15 ohm-cm | IEC 60093 |
Raschig Group 3536 Epoxy Glass-fiber reinforced epoxy molding compound. Good mechanical strength, very good electrical isolation properties and dimensional stability even at high temperatures. This product meets the allowed.. |
|||
Volume Resistivity | 1.00e+14 - 1.00e+15 ohm-cm | 1.00e+14 - 1.00e+15 ohm-cm | IEC 60093 |
Raschig Group 4554 Silicone Glass fiber reinforced silicone molding compound. Excellent thermal stability - up to 300°C, exceptional electrical properties, good mechanical strength, very good dimensional stability. Processi.. |
|||
Volume Resistivity | 1.00e+14 - 1.00e+15 ohm-cm | 1.00e+14 - 1.00e+15 ohm-cm | IEC 60093 |
Raschig Group 5563 DAP Glass-fiber reinforced diallyl phthalate molding compound. Good mechanical strength together with retention of high electrical isolation properties under hot humid conditions, exceptional dimensiona.. |
|||
Volume Resistivity | 1.00e+14 - 1.00e+15 ohm-cm | 1.00e+14 - 1.00e+15 ohm-cm | IEC 60093 |
Raschig Group 6552 DAIP Glass-fiber reinforced diallyl isophthalate molding compound. Good mechanical strength together with retention of high electrical isolation properties under hot humid conditions, exceptional dimensi.. |
|||
Volume Resistivity | 1.00e+14 - 1.00e+15 ohm-cm | 1.00e+14 - 1.00e+15 ohm-cm | IEC 60093 |
Raschig Group RALUPOL® 4385 UP Glass-fiber reinforced polyester molding compound. Low mold shrinkage and post-shrinkage, very high arc resistance, very high mechanical values. This product meets the allowed upper limits for heavy.. |
|||
Volume Resistivity | 1.00e+14 - 1.00e+15 ohm-cm | 1.00e+14 - 1.00e+15 ohm-cm | IEC 60093 |
Raschig Group RALUPOL® 4806 UP Glass-fiber reinforced polyester molding compound. Very low mold shrinkage and post-shrinkage, very good mechanical strength, very good electrical values, better performance values compared to UP 80.. |
|||
Volume Resistivity | 1.00e+14 - 1.00e+15 ohm-cm | 1.00e+14 - 1.00e+15 ohm-cm | IEC 60093 |
Raschig Group 3572 Epoxy Glass-fiber reinforced epoxy molding compound. Good mechanical strength and electrical strength, enhanced elasticity for ensuring good sealing under extreme heat and/or humidity, good chemical resis.. |
|||
Volume Resistivity | 1.00e+14 - 1.00e+15 ohm-cm | 1.00e+14 - 1.00e+15 ohm-cm | IEC 60093 |
Raschig Group SURAPLAST 54 UPA Glass fiber reinforced polyester molding compound. Minimal mold shrinkage and post-shrinkage, very good arc resistance, very good mechanical strength. This product meets the allowed upper limits for.. |
|||
Volume Resistivity | 1.00e+14 - 1.00e+15 ohm-cm | 1.00e+14 - 1.00e+15 ohm-cm | IEC 60093 |
Raschig Group SURAPLAST UPA 63 UP Glass fiber reinforced polyester molding compound. Minimal mold shrinkage and post-shrinkage, very good arc resistance, very good mechanical strength. This product meets the allowed upper limits for.. |
|||
Volume Resistivity | 1.00e+14 - 1.00e+15 ohm-cm | 1.00e+14 - 1.00e+15 ohm-cm | ASTM D257 |
Supreme Petrochem SP 6530 Antistatic Polystyrene Characteristics Prevents dust patterns due to static charges Eliminates need of coatings Fully colorable Processing Injection molding Extrusion & Forming Applications Meter housings Foodservice .. |
|||
Volume Resistivity | 1.00e+13 - 1.00e+15 ohm-cm | 1.00e+13 - 1.00e+15 ohm-cm | ASTM D257 |
Eastman Tenite 285E0V16304 Cellulose Acetate Butyrate, Clear, Trsp Applications:DisplaysProduct Description: Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. T.. |
|||
Volume Resistivity | 1.00e+13 - 1.00e+15 ohm-cm | 1.00e+13 - 1.00e+15 ohm-cm | ASTM D257 |
Eastman Tenite 307E0V16310 Propionate Clear, Trsp Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. The mechanical properties if Tenite cellulosi.. |
|||
Volume Resistivity | 1.00e+13 - 1.00e+15 ohm-cm | 1.00e+13 - 1.00e+15 ohm-cm | ASTM D257 |
Eastman Tenite 350A0096914 Propionate Natural Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. The mechanical properties of Tenite cellulosi.. |
|||
Volume Resistivity | 1.00e+13 - 1.00e+15 ohm-cm | 1.00e+13 - 1.00e+15 ohm-cm | ASTM D257 |
Eastman Tenite 350A4861313 Cellulose Acetate Propionate, Clear, Trsp Applications:Blood TherapyDrug DeliveryIV ComponentsMedical DevicesSurgical InstrumentsProduct Description: Tenite cellulosic plastics are noted for their excellent balance of properties - toughne.. |
|||
Volume Resistivity | 1.00e+13 - 1.00e+15 ohm-cm | 1.00e+13 - 1.00e+15 ohm-cm | ASTM D257 |
Eastman Tenite 360A4000012 Propionate Clear, Trsp Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. The mechanical properties if Tenite cellulosi.. |
|||
Volume Resistivity | 1.00e+13 - 1.00e+15 ohm-cm | 1.00e+13 - 1.00e+15 ohm-cm | ASTM D257 |
Eastman Tenite 360E2R30016 Cellulose Acetate Propionate, Natural, Trsp Applications:AppliancesPersonal Care and CosmeticsProduct Description: Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss.. |
|||
Volume Resistivity | 1.00e+13 - 1.00e+15 ohm-cm | 1.00e+13 - 1.00e+15 ohm-cm | ASTM D257 |
Eastman Tenite 360E3V45516 Propionate Water Clear, Trsp Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. The mechanical properties of Tenite cellulosi.. |
|||
Volume Resistivity | 1.00e+13 - 1.00e+15 ohm-cm | 1.00e+13 - 1.00e+15 ohm-cm | ASTM D257 |
Eastman Tenite 371A2R30008 Cellulose Acetate Propionate, Natural, Trsp Applications:Consumer-Personal CareToothbrushesProduct Description: Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, c.. |
|||
Volume Resistivity | 1.00e+13 - 1.00e+15 ohm-cm | 1.00e+13 - 1.00e+15 ohm-cm | ASTM D257 |
Eastman Tenite 371A4000012 Cellulose Acetate Propionate, Clear, Trsp Applications:OphthalmicsOral HygienePen/stationary suppliesToothbrushesProduct Description: Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, st.. |
|||
Volume Resistivity | 1.00e+13 - 1.00e+15 ohm-cm | 1.00e+13 - 1.00e+15 ohm-cm | ASTM D257 |
Eastman Tenite 380A3V32818 Propionate Clear, Trsp Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. The mechanical properties if Tenite cellulosi.. |
|||
Volume Resistivity | 1.00e+13 - 1.00e+15 ohm-cm | 1.00e+13 - 1.00e+15 ohm-cm | ASTM D257 |
Eastman Tenite 380A4000015 Cellulose Acetate Propionate, Clear, Trsp Applications:OphthalmicsProduct Description: Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel.. |
|||
Volume Resistivity | 1.00e+14 - 1.00e+15 ohm-cm @Temperature 23.0 °C |
1.00e+14 - 1.00e+15 ohm-cm @Temperature 73.4 °F |
ASTM D257 |
Daelim H&L Plavis G15 Aromatic Polyimide, 15% Graphite Filled, Machined Parts High abrasion resistance, very low friction coefficient property, suitable for being applied to spin component of spin apparatusInformation provided by Daelim H&L |
|||
Volume Resistivity | 1.00e+12 - 1.00e+15 ohm-cm | 1.00e+12 - 1.00e+15 ohm-cm | DIN 53 482, VDE 0303, Part 3 |
Hippe PA 66 Nylon 66 The polyamide with high degree of hardness, stiffness, scuff strength and stability of shape under heat. Preferred polyamide for components subjected to high load and heat stress in electrical, mec.. |
|||
Volume Resistivity | 1.00e+14 - 1.00e+15 ohm-cm | 1.00e+14 - 1.00e+15 ohm-cm | IEC 60093 |
Raschig Group 5567 DAP Diallyl Phthalate (DAP), Cast, Mineral Filler Glass-fiber reinforced diallyl phthalate molding compound free from halogens. Good mechanical strength together with retention of high electrical isolation properties under hot humid conditions, exc.. |
|||
Volume Resistivity | 1.00e+14 - 1.00e+15 ohm-cm | 1.00e+14 - 1.00e+15 ohm-cm | IEC 60093 |
Raschig Group RALUPOL® 8605 UP Polyester Glass fiber reinforced polyester molding compound. Resistant to hydrolysis. This product meets the allowed upper limits for heavy metals and PCAs and also conforms to the requirements of the EU dire.. |
|||
Volume Resistivity | 1.00e+13 - 1.00e+15 ohm-cm | 1.00e+13 - 1.00e+15 ohm-cm | ASTM D257 |
Eastman Tenite 550E3V45510 Butyrate Water Clear, Trsp
(discontinued **) Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. The mechanical properties of Tenite cellulosi.. |
|||
Volume Resistivity | 1.00e+13 - 1.00e+15 ohm-cm | 1.00e+13 - 1.00e+15 ohm-cm | ASTM D257 |
Eastman Tenite 360A4861301 Propionate Clear, Trsp
(discontinued **) Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. The mechanical properties if Tenite cellulosi.. |