Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 2.00e+16 ohm-cm | 2.00e+16 ohm-cm | ASTM D257 |
Solvay Specialty Polymers Udel® GF-120 Polysulfone (PSU)
(Unverified Data**) Udel GF-120, resin is a 20% glass fiber reinforced polysulfone compound. Glass fiber substantially increases the rigidity, tensile strength, creep resistance, dimensional stability and chemical resi.. |
|||
Volume Resistivity | 2.00e+16 ohm-cm | 2.00e+16 ohm-cm | ASTM D257 |
Solvay Specialty Polymers Udel® GF-130 Polysulfone (PSU)
(Unverified Data**) Udel GF-130, resin is a 30% glass fiber reinforced polysulfone compound. Glass fiber substantially increases the rigidity, tensile strength, creep resistance, dimensional stability and chemical resi.. |
|||
Volume Resistivity | 2.00e+16 ohm-cm | 2.00e+16 ohm-cm | IEC 60093 |
Ineos ABS Lustran® M205FC ABS Pellets, Injection Molding Grade Injection Molding grade for medical applications (e.g. inhalers, roller clamps, spikes, etc.)/ Biocompatible with up to 30 days human contact duration according to USP Class VI and ISO 10993-1. Food.. |
|||
Volume Resistivity | 2.00e+16 ohm-cm | 2.00e+16 ohm-cm | ASTM D257 |
SABIC Innovative Plastics NORYL PX9406 PPE+PS (Asia Pacific) Nonbrominated, nonchlorinated, flame retarded. Improved productivity and reliability. 252F HDT. UL94 V-0 rated. Electrical applications. |
|||
Volume Resistivity | 2.00e+16 ohm-cm | 2.00e+16 ohm-cm | 500V; Ø 93x3mm; IEC 60093 |
SYNTHOS Forsan® 573 L Acrylonitrile Butadiene Styrene (ABS) Increased heat resistant, glossy, UV stabilized.Applications: Electrotechnics, automotiveHousehold appliances, office equipment, car interior parts, profiles, ABS sheets, etc.Synthos was formerly kn.. |
|||
Volume Resistivity | 2.00e+16 ohm-cm | 2.00e+16 ohm-cm | ASTM D257 |
Solvay Specialty Polymers Udel® GF-120 Polysulfone (PSU), Glass Fiber Udel® GF-120, resin is a 20% glass fiber reinforced polysulfone compound. Glass fiber substantially increases the rigidity, tensile strength, creep resistance, dimensional stability and chemical .. |
|||
Volume Resistivity | 2.00e+16 ohm-cm | 2.00e+16 ohm-cm | ASTM D257 |
Techmer ES HiFill® PP LGF50 CC NAT 12mm 50% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Long Glass Fiber, 50% Filler by WeightFeatures: Chemically CoupledInformation provided by TP Composites, Inc. |
|||
Volume Resistivity | 2.00e+16 ohm-cm | 2.00e+16 ohm-cm | GB/T1410-2006 |
Sichuan Deyang Haton® hGR40 Polyphenylene Sulfide, Glass Fiber Reinforced Injection moldingInformation provided by Sichuan Deyang Chemical Co., LTD |
|||
Volume Resistivity | >= 2.00e+16 ohm-cm | >= 2.00e+16 ohm-cm | IEC 60093 |
Styrolution Novodur® M205FC ABS Novodur HD M205FC is an injection molding grade especially suitable for medical applications providing enhanced stiffness.Information provided by Styrolution |
|||
Volume Resistivity | 2.00e+16 ohm-cm | 2.00e+16 ohm-cm | ASTM D257 |
Techmer ES HiFill FR® PC GF20 FR 20% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 20% Filler by WeightFeatures: Flame RetardantInformation provided by TP Composites, Inc. |
|||
Volume Resistivity | 2.00e+16 ohm-cm | 2.00e+16 ohm-cm | IEC 60093 |
Polyplastics Duranex® 733LD Polybutylene Terephthalate (PBT), Low warpage, 30% GF filled DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers .. |
|||
Volume Resistivity | 2.00e+16 ohm-cm | 2.00e+16 ohm-cm | IEC 60093 |
Polyplastics FR-PET® BLR6001MZ Glass Fiber Reinforced Polyethylene Terephthalate (GF-PET) Information provided by PolyPlastics. |
|||
Volume Resistivity | 2.00e+16 ohm-cm | 2.00e+16 ohm-cm | 50% RH; tested on 10 mil thickness sample; ASTM D257 |
DuPont™ Nomex® 410 Paper, 2 mil Nominal Thickness Nomex® Type 410 is a calendared insulation paper which offers high inherent dielectric strength, mechanical toughness, flexibility, and resilience. It is the original form of Nomex® paper and is .. |
|||
Volume Resistivity | 2.00e+16 ohm-cm | 2.00e+16 ohm-cm | 50% RH; tested on 10 mil thickness sample; ASTM D257 |
DuPont™ Nomex® 410 Paper, 20 mil Nominal Thickness Nomex® Type 410 is a calendared insulation paper which offers high inherent dielectric strength, mechanical toughness, flexibility, and resilience. It is the original form of Nomex® paper and is .. |
|||
Volume Resistivity | 2.00e+16 ohm-cm | 2.00e+16 ohm-cm | 50% RH; tested on 10 mil thickness sample; ASTM D257 |
DuPont™ Nomex® 410 Paper, 24 mil Nominal Thickness Nomex® Type 410 is a calendared insulation paper which offers high inherent dielectric strength, mechanical toughness, flexibility, and resilience. It is the original form of Nomex® paper and is .. |
|||
Volume Resistivity | 2.00e+16 ohm-cm | 2.00e+16 ohm-cm | 50% RH; tested on 10 mil thickness sample; ASTM D257 |
DuPont™ Nomex® 410 Paper, 29 mil Nominal Thickness Nomex® Type 410 is a calendared insulation paper which offers high inherent dielectric strength, mechanical toughness, flexibility, and resilience. It is the original form of Nomex® paper and is .. |
|||
Volume Resistivity | 2.00e+16 ohm-cm | 2.00e+16 ohm-cm | 50% RH; tested on 10 mil thickness sample; ASTM D257 |
DuPont™ Nomex® 410 Paper, 7 mil Nominal Thickness Nomex® Type 410 is a calendared insulation paper which offers high inherent dielectric strength, mechanical toughness, flexibility, and resilience. It is the original form of Nomex® paper and is .. |
|||
Volume Resistivity | >= 2.00e+16 ohm-cm | >= 2.00e+16 ohm-cm | ASTM D257 |
Fainplast Compounds Ethylplus 613 HPE Polyethylene Cable Compound Polyethelene, halogen-free cable compound with superior thermo-mechanical properties, outstanding heat resistance, and high electrical propertiesExpandable HDPE by gas injectionInformation provided .. |
|||
Volume Resistivity | 2.00e+16 ohm-cm @Thickness 2.00 mm |
2.00e+16 ohm-cm @Thickness 0.0787 in |
ASTM D257 |
Beijing Ranger Chem PBT 403 M-G30 HF Halogen Free Flame Retarding FR PBT Modified PBT Characteristics: Unreinforced grades have abundant strength and flexibility, and have strong characteristics against brittleness. UL-certified slow-burning (94HB) and self-extinguishin.. |
|||
Volume Resistivity | 2.00e+16 ohm-cm | 2.00e+16 ohm-cm | ASTM D257 |
BLUESTAR 403HF-G20 PBT, 20% Glass Filled Typical Applications: Halogen Free; E/E connectors, socketsInformation provided by Polymer Technology and Services, LLC (PTS). |
|||
Volume Resistivity | 2.00e+16 ohm-cm | 2.00e+16 ohm-cm | 50% RH |
Parylene Coating Services D Poly (P-Xylylene) Monomer is dichloro para-xylylene. Parylene D is recommended where high temperature resistance is needed; it can be used up to 140°C where oxygen is present.Parylene is a generic name for poly-par.. |
|||
Volume Resistivity | 2.00e+16 ohm-cm | 2.00e+16 ohm-cm | ASTM D257 |
Solvay Specialty Polymers Amodel® AS-4133 HN Polyphthalamide (PPA), Dry, 33% Glass Fiber Reinforcement, Heat Stabilizer Amodel AS-4133 HN polyphthalamide (PPA) is a non-lubricated, heat stabilized grade that offers fast cycle times and is hot-water moldable. Typical applications include electrical and electronic comp.. |