Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 2.00e+13 ohm-cm | 2.00e+13 ohm-cm | Z direction; C96/35/90; ASTM D257 |
Rogers Corporation RT/duroid® 5880 Glass Microfiber Reinforced PTFE High Frequency Laminate RT/duroid® 5870 and 5880 glass microfiber reinforced PTFE composites are designed for exacting stripline and microstrip circuit applications. Glass reinforcing microfibers are randomly oriented to.. |
|||
Volume Resistivity | 2.00e+13 ohm-cm | 2.00e+13 ohm-cm | ASTM D257 |
Permabond TA435 Toughened Acrylic Adhesive & Initiator PERMABOND TA435 is a structural acrylic adhesive designed primarily for bonding metals, ferrites, ceramics and some thermoplastics. This adhesive may be used in a variety of structural bonding appli.. |
|||
Volume Resistivity | 2.00e+13 ohm-cm | 2.00e+13 ohm-cm | ASTM D257 |
Permabond TA437 Toughened Acrylic Adhesive PERMABOND TA437 is a single component structural acrylic adhesive designed primarily for bonding metals, ferrites and ceramics. The typical fixture time of TA437 when used with Initiator 41 is 30 –.. |
|||
Volume Resistivity | 2.00e+13 ohm-cm | 2.00e+13 ohm-cm | ASTM D257 |
Permabond TA439 Toughened Acrylic Adhesive Permabond® TA439 is a two component structural acrylic adhesive designed primarily for bonding metals, ferrites, ceramics and some plastics. The typical fixture time of is 10-30 seconds. The fast f.. |
|||
Volume Resistivity | 2.00e+13 ohm-cm | 2.00e+13 ohm-cm | ASTM D257 |
Permabond TA440 Toughened Acrylic Adhesive PERMABOND TA440 is a two component structural acrylic adhesive suitable for bonding metals, glass, wood, ferrites, ceramics and some rigid plastics. This adhesive may be used in a variety of structu.. |
|||
Volume Resistivity | 2.00e+13 ohm-cm | 2.00e+13 ohm-cm | ASTM D257 |
Permabond TA4302 Toughened Acrylic Adhesive PERMABOND® TA4302 is a 2-part, 1:1 toughened acrylic adhesive. It can be used to bond a wide variety of materials including metals, plastics, GRP, ceramics, wood and other substrates. It is conveni.. |
|||
Volume Resistivity | 2.00e+13 ohm-cm | 2.00e+13 ohm-cm | 60°C for 500 hrs with 95% RH |
Fujipoly Industries Sarcon® 85U Thin-Film UR Sarcon UR is Fujipolys originally developed High Heat Conductive/Low Hardness Silicone Rubber. Fine, high heat conductive ceramic particles are mixed with insulative silicone rubber.Information prov.. |
|||
Volume Resistivity | 2.00e+13 ohm-cm | 2.00e+13 ohm-cm | 60°C for 500 hrs with 90% RH; JIS-K-6249 |
Fujipoly Industries Sarcon® GR-b Gap Filler Pad Sarcon GR-b is a highly conformable, thermally conductive material in areas where space between surfaces is uneven and surface textures vary.Information provided by Fujipoly Industries |
|||
Volume Resistivity | 2.00e+13 ohm-cm | 2.00e+13 ohm-cm | ASTM D257 |
Techmer ES Elastoblend® PA6 IM 409 L MB Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer, Impact Modifier and LubricantFeatures: Heat Stabilized, Impact Modified and LubricatedInformation provided by TP Composites, Inc. |
|||
Volume Resistivity | 2.00e+13 ohm-cm | 2.00e+13 ohm-cm | ASTM D257 |
Techmer ES Elastoblend® PA6 IM 511 HS L Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer, Impact Modifier and LubricantFeatures: Heat Stabilized, Impact Modified and LubricatedUses: Low Temperature ApplicationsInformatio.. |
|||
Volume Resistivity | 2.00e+13 ohm-cm | 2.00e+13 ohm-cm | ASTM D257 |
Techmer ES Elastoblend® PA6 IM L N Availability: North AmericaForms: PelletsAdditive: Impact Modifier and LubricantFeatures: Impact Modified and LubricatedAppearance: Natural ColorInformation provided by TP Composites, Inc. |
|||
Volume Resistivity | 2.00e+13 ohm-cm | 2.00e+13 ohm-cm | ASTM D257 |
Techmer ES Elastoblend® PA6 IM X Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer, Impact Modifier and LubricantFeatures: Heat Stabilized, Impact Modified and LubricatedProcessing Method: Injection MoldingInformat.. |
|||
Volume Resistivity | 2.00e+13 ohm-cm | 2.00e+13 ohm-cm | ASTM D257 |
Techmer ES Plastiblend® PA6/ABS 1120 B1 Availability: North AmericaForms: PelletsAdditive: Impact ModifierFeatures: Impact ModifiedUL File Number: E157318Information provided by TP Composites, Inc. |
|||
Volume Resistivity | 2.00e+13 ohm-cm | 2.00e+13 ohm-cm | IEC 60093 |
Solvay TECHNYL® A 216 V33 PA66, 33% glass fiber, Conditioned Description: TECHNYL® A 216 V33 is a polyamide 66, reinforced with 33% of glass fiber, for injection molding. This product is available in natural color.Benefits: The product offers an excellent .. |
|||
Volume Resistivity | 2.00e+13 ohm-cm | 2.00e+13 ohm-cm | IEC 60093 |
Unitika A1030GFL45 PA6, 45% Glass Fiber Reinforced, Dry Information provided by Unitika Ltd. |
|||
Volume Resistivity | 2.00e+13 ohm-cm | 2.00e+13 ohm-cm | IEC 60093 |
Unitika A3130 PA6, 35% Mineral Reinforced, Dry Information provided by Unitika Ltd. |
|||
Volume Resistivity | 2.00e+13 ohm-cm | 2.00e+13 ohm-cm | ASTM D257 |
Toyobo PELPRENE™ S2001 Polyester TPE Features: Polyester TPEInformation provided by Toyobo. |
|||
Volume Resistivity | 2.00e+13 ohm-cm | 2.00e+13 ohm-cm | ASTM D257 |
Toyobo PELPRENE™ S2002 Polyester TPE, Ultra Heat-resistant Features: Polyester TPE, Ultra Heat-resistantInformation provided by Toyobo. |
|||
Volume Resistivity | 2.00e+13 ohm-cm | 2.00e+13 ohm-cm | ASTM D257 |
Toyobo PELPRENE™ S2004FS Polyester TPE, Flame Resistant Features: Polyester TPE, Flame ResistantInformation provided by Toyobo. |
|||
Volume Resistivity | <= 2.00e+13 ohm-cm | <= 2.00e+13 ohm-cm | |
Epoxy Technology EPO-TEK® 305 Spectrally Transparent Epoxy Product Description: EPO-TEK® 305 is a two component, semi-rigid, optical grade epoxy for semiconductor packaging of fiber optics, optoelectronics and medical devices. It is an electrically and th.. |
|||
Volume Resistivity | <= 2.00e+13 ohm-cm | <= 2.00e+13 ohm-cm | |
Epoxy Technology EPO-TEK® 360T High Temperature Epoxy Material Description: A two component, high-temperature grade, electrically and thermally insulating epoxy for semiconductor, electronics, fiber optics and medical applications. It is a thixotropic.. |
|||
Volume Resistivity | 2.00e+13 ohm-cm @Temperature 23.0 °C |
2.00e+13 ohm-cm @Temperature 73.4 °F |
ASTM D257 |
Fainplast Compounds AP 88/1 Flexible PVC, Flame Retardant Insulation General purposes |
|||
Volume Resistivity | 2.00e+13 ohm-cm | 2.00e+13 ohm-cm | |
Resinlab® EP1310 Medium Reactivity Epoxy Encapsulant Resinlab™ EP1310 is a two part medium reactivity epoxy encapsulant capable of being quickly gelled prior to full cure by exposing to a UV light source. Usually 5- 10 seconds is sufficient to gel th.. |