Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 1.00e+18 ohm-cm | 1.00e+18 ohm-cm | IEC 60093 |
3M Dyneon™ TFX 2035 PTFE
(discontinued **) Typical Applications: Liners, extruded tape, thick wall tubing.Information provided by the Dyneon division of 3M. |
|||
Volume Resistivity | 1.00e+18 ohm-cm | 1.00e+18 ohm-cm | ASTM D257 |
Techmer ES HiFill FR® PC FR SFX-ORANGE 1.0 Availability: North AmericaForms: PelletsAdditive: UV StabilizerFeatures: Flame RetardantAppearance: OrangeInformation provided by TP Composites, Inc. |
|||
Volume Resistivity | 1.00e+18 ohm-cm | 1.00e+18 ohm-cm | ASTM D257 |
Techmer ES Plastiblend® PC/ABS FR 2810 Availability: North AmericaForms: PelletsFeatures: Flame RetardantInformation provided by TP Composites, Inc. |
|||
Volume Resistivity | >= 1.00e+18 ohm-cm | >= 1.00e+18 ohm-cm | IEC 60093 |
Styrolution Novodur® BX13036 ABS + PMMA Novodur BX13036 is a new PMMA/ABS blend with high surface quality, enhanced scratch resistance and balanced mechanical propertiesInformation provided by Styrolution |
|||
Volume Resistivity | >= 1.00e+18 ohm-cm | >= 1.00e+18 ohm-cm | IEC 60093 |
Styrolution PS 156F GPPS Styrolution PS 156F is a general purpose polystyrene grade with excellent flow properties, high heat resistance and is zinc stearate free.Free of internal lubricantsHigh heat resistanceExcellent flo.. |
|||
Volume Resistivity | >= 1.00e+18 ohm-cm | >= 1.00e+18 ohm-cm | IEC 60093 |
Styrolution PS 416N HIPS Styrolution PS 416N is medium impact polystyrene with very good flow properties. It has a high rigidity whilst displaying a very good surface gloss.Very good flow propertiesHigh rigidityVery good su.. |
|||
Volume Resistivity | >= 1.00e+18 ohm-cm | >= 1.00e+18 ohm-cm | IEC 60093 |
Styrolution PS 454N HIPS Styrolution PS 454N is an impact resistant polystyrene with a good balance of toughness, high flow, heat resistance and high gloss.Good balance of toughness, high flow, and heat resistanceHigh gloss.. |
|||
Volume Resistivity | >= 1.00e+18 ohm-cm | >= 1.00e+18 ohm-cm | IEC 60093 |
Styrolution PS 576H HIPS Styrolution PS 576H is a high gloss, high impact polystyrene with a good flow and good heat resistance.High gloss HIPSGood flow and heat resistanceHIPS with good balance of mechanical properties and.. |
|||
Volume Resistivity | 1.00e+18 ohm-cm | 1.00e+18 ohm-cm | ASTM D257 |
Teknor Apex Chemlon® 100 W Nylon 66, Unreinforced Notes: MoS2 modified; Molybdenum disulphide modified to provide self-lubrication and low friction to parts subjected to wear and abrasion. FMVSS Flammability: Passes, FMVSS 302Processing Method: Inj.. |
|||
Volume Resistivity | >= 1.00e+18 ohm-cm | >= 1.00e+18 ohm-cm | IEC 60093 |
Styrolution PS 158K GPPS Styrolution PS 158K is a heat resistant, rapid freezing general purpose grade. It is suitable for expanded sheet and film; for blends with high impact Styrolution PS in heat contact applications; fo.. |
|||
Volume Resistivity | 1.00e+18 ohm-cm | 1.00e+18 ohm-cm | ASTM D257 |
Dalau Dalcon 086 100% Virgin PTFE modified polymer Applications & Industries: General: The static and dynamic friction coefficient are numerically equal, consequently no ’Stick Slip’ occurs. Modified PTFE has an advantage over Homopolymer (Normal .. |
|||
Volume Resistivity | 1.00e+18 ohm-cm | 1.00e+18 ohm-cm | D257 |
Zhejiang Juner JEPP263 Weatherability PP Series Applications: Air Conditioning SystemInformation provided by Zhejiang Juner New Materials Co, Ltd. |
|||
Volume Resistivity | 1.00e+18 ohm-cm | 1.00e+18 ohm-cm | D257 |
Zhejiang Juner JEPPB005 High Glossy PP Applications: Shell of Air ConditionerInformation provided by Zhejiang Juner New Materials Co, Ltd. |
|||
Volume Resistivity | 1.00e+18 ohm-cm | 1.00e+18 ohm-cm | D257 |
Zhejiang Juner JEPPBC001 Weatherability PP Series Applications: Weatherability ProductsInformation provided by Zhejiang Juner New Materials Co, Ltd. |
|||
Volume Resistivity | 1.00e+18 ohm-cm | 1.00e+18 ohm-cm | D257 |
Zhejiang Juner PP201-G30 PP For Automotive Parts Applications: FansInformation provided by Zhejiang Juner New Materials Co, Ltd. |
|||
Volume Resistivity | 1.00e+18 ohm-cm | 1.00e+18 ohm-cm | D257 |
Zhejiang Juner PP430R Weatherability PP Series Applications: Air Conditioning SystemInformation provided by Zhejiang Juner New Materials Co, Ltd. |
|||
Volume Resistivity | 1.00e+18 ohm-cm | 1.00e+18 ohm-cm | D257 |
Zhejiang Juner PP6-1JE PP For Automotive Parts Applications: Air Conditioning SystemInformation provided by Zhejiang Juner New Materials Co, Ltd. |
|||
Volume Resistivity | <= 1.00e+18 ohm-cm | <= 1.00e+18 ohm-cm | ASTM D257 |
Daikin NEOFLON NP-21 FEP Pellets NEOFLON FEP molding materials are supplied as translucent white pellets for melt flow processes.Processing Methods: Extrusion molding, injection molding.Applications: Suited to high speed extrusion .. |
|||
Volume Resistivity | <= 1.00e+18 ohm-cm | <= 1.00e+18 ohm-cm | ASTM D257 |
Daikin NEOFLON NP-30 FEP Pellets NEOFLON FEP molding materials are supplied as translucent white pellets for melt flow processes.Processing Methods: Extrusion molding.Applications: Heavy wall wire insulation, tubes, cable jacketing.. |
|||
Volume Resistivity | <= 1.00e+18 ohm-cm | <= 1.00e+18 ohm-cm | ASTM D257 |
Daikin NEOFLON NP-40 FEP Pellets NEOFLON FEP molding materials are supplied as translucent white pellets for melt flow processes.Processing Methods: Extrusion molding, transfer molding, compression molding.Applications: Films and s.. |
|||
Volume Resistivity | <= 1.00e+18 ohm-cm | <= 1.00e+18 ohm-cm | ASTM D257 |
Daikin POLYFLON MG-1030 PTFE 15% Glass Fiber Filled Molding Powder 15% glass fiber filled. High wear resistance, low friction, good electrical properties.Applications: Mechanical and electrical service. Available in all forms (e.g. bearings, gaskets, valve seats,.. |
|||
Volume Resistivity | <= 1.00e+18 ohm-cm | <= 1.00e+18 ohm-cm | ASTM D257 |
Daikin POLYFLON MG-1431F PTFE 20% Glass Fiber and 5% MoS2 Filled Molding Powder, High Apparent Density, Free Flow 15% glass fiber and 5% MoS2 filled. High apparent density and free-flowing properties. High wear resistance, good electrical properties, low friction, high creep resistance.Applications: Mechanica.. |
|||
Volume Resistivity | <= 1.00e+18 ohm-cm | <= 1.00e+18 ohm-cm | ASTM D257 |
Daikin NEOFLON AP-201 PFA Pellets NEOFLON PFA pellets have good melt flowability, and can be processed in the same manner as other thermoplastic resins.Applications: Complicated injection molded parts requiring high melt flow to fil.. |
|||
Volume Resistivity | 1.00e+18 ohm-cm | 1.00e+18 ohm-cm | ASTM D257 |
Adamas Adalon® 433 PTFE, 10% Ekonol® Information provided by Adamas, HPM |
|||
Volume Resistivity | >= 1.00e+18 ohm-cm | >= 1.00e+18 ohm-cm | ASTM D257 |
Asahi Glass Fluon® P-66P PFA Perfluoropolymer Fluon® PFA is a copolymer of tetrafluoroethylene (C2F4) and perfluoroalkoxyethylene, which has excellent chemical, electrical, mechanical and surface properties. PFA retains many inherent character.. |
|||
Volume Resistivity | >= 1.00e+18 ohm-cm | >= 1.00e+18 ohm-cm | ASTM D257 |
Asahi Glass Fluon® P-63P PFA Perfluoropolymer Fluon® PFA is a copolymer of tetrafluoroethylene (C2F4) and perfluoroalkoxyethylene, which has excellent chemical, electrical, mechanical and surface properties. PFA retains many inherent character.. |
|||
Volume Resistivity | 1.00e+18 ohm-cm | 1.00e+18 ohm-cm | STN 34 6460 |
Plastcom SLOVASTER® B GB 40 PBT reinforced with glass beads PBT for injection molding, reinforced with 40% glass beads. Characterized by very good properties also at low temperature. Melt is characterized by very good rheology, which enables manufacturing of.. |