Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 1.00e+14 ohm-cm | 1.00e+14 ohm-cm | IEC 60093 |
DSM Akulon® Ultraflow™ K-FHGM24 Nylon 6-30% Glass and Mineral Reinforced (European Grade) (Dry)
(discontinued The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
Volume Resistivity | 1.00e+14 ohm-cm | 1.00e+14 ohm-cm | ASTM D257 |
Kingfa HF-626 Flame Retardant ABS Features:UL 94 V-0 @ 1.6-3.0mm, 5VB @ 2.0mmHigh flowHigh impact resistanceApplications:Injection moldingMonitor cabinetCD-ROMPower switchInformation Provided by Kingfa Sci. & Tech. Co., Ltd. |
|||
Volume Resistivity | 1.00e+14 ohm-cm | 1.00e+14 ohm-cm | ASTM D257 |
LG Chemical LUCEL N127LD POM, Chemical Resistance Feature: Injection Molding, POM, Chemical ResistanceApplication: Copier, Watch, Clock, VCR, Printer Parts, etc.CAS No. 66455-31-0Information provided by LG Chemical |
|||
Volume Resistivity | 1.00e+14 ohm-cm | 1.00e+14 ohm-cm | ASTM D257 |
Kolon KOCETAL® K200 Standard Grade Acetal Resin Suitable for both injection and extrusion.Applications: Injection and extruded use such as rod and sheetInformation provided by API Kolon. |
|||
Volume Resistivity | 1.00e+14 ohm-cm | 1.00e+14 ohm-cm | ASTM D257 |
LG Chemical LUMID SG4389B PA66+GF/MF38% Feature: Injection Molding, PA66+GF/MF38%Application: Automotive (Fan & Shroud)CAS No. 32131-17-2, 25038-54-4, 65997-17-3 and 14807-96-6Information provided by LG Chemical |
|||
Volume Resistivity | >= 1.00e+14 ohm-cm | >= 1.00e+14 ohm-cm | ASTM D 257 |
Karina 18/335-FC Gray Color Concentrate for PVC Color concentrate recommended for application in electrical wire and cable PVC compounds. Also suitable for pigmentation of flexible and rigid PVC compounds for general purposes. Recommended to use.. |
|||
Volume Resistivity | >= 1.00e+14 ohm-cm | >= 1.00e+14 ohm-cm | NBR 5403 |
Karina E 42/268-FC-LMP Red Color Concentrate for PVC Color concentrate recommended for application in PVC compounds for electrical wires and cables. Also suitable for pigmentation of flexible and rigid PVC compounds for general purposes.Important con.. |
|||
Volume Resistivity | 1.00e+14 ohm-cm | 1.00e+14 ohm-cm | |
LG Chemical AF305HT ABS, Flame Retardant, Heat Resistance Feature: Injection Molding, Flame Retardant, Heat ResistanceApplication: Electric/Electronic Applications (TV, Monitor Housing) IT/OA deviceCAS No. 9003-56-9, 9001-96-2, 68928-70-1, and 1309-64-4Inf.. |
|||
Volume Resistivity | 1.00e+14 ohm-cm | 1.00e+14 ohm-cm | IEC 60093 |
Solvay TECHNYL® A 402 Natural FA PA66, DRY Description: Unreinforced polyamide PA66, very high viscosity, for extrusion.Available in: Europe and North AmericaProduct Applications: TECHNYL® A 402 NATURAL FA offers three main advantages: hi.. |
|||
Volume Resistivity | 1.00e+14 ohm-cm | 1.00e+14 ohm-cm | ASTM D257 |
Techmer ES HiFill FR® PA6 GF33 FR HS L BK065 33% Glass Filled (Dry) Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 33% Filler by WeightAdditive: Heat Stabilizer and LubricantFeatures: Flame Retardant, Heat Stabilized and Lu.. |
|||
Volume Resistivity | 1.00e+14 ohm-cm | 1.00e+14 ohm-cm | ASTM D257 |
Techmer ES HiFill FR® PA6/6 GF33 FR-N BK 33% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 30% Filler by WeightFeatures: Flame Retardant and Halogen FreeAppearance: BlackInformation provided by TP Composites, Inc... |
|||
Volume Resistivity | 1.00e+14 ohm-cm | 1.00e+14 ohm-cm | ASTM D257 |
SABIC Innovative Plastics Valox® ENH4560 PBT (Europe-Africa-Middle East) Valox* ENH4560 resin is a non-brominated/non-chlorinated flame retardant product based on Valox* PBT resin. |
|||
Volume Resistivity | 1.00e+14 ohm-cm | 1.00e+14 ohm-cm | ASTM D257 |
Techmer ES Luriblend® PA6/6 04003 Nylon 66 Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer and Molybdenum Disulfide Lubricant(15%)Features: Lubricated, Good Wear Resistance, Low Friction and Heat StabilizedAppearance: Natu.. |
|||
Volume Resistivity | 1.00e+14 ohm-cm | 1.00e+14 ohm-cm | DIN 53482 |
Polyram RamTal PM3009G5 Acetal, 25% Glass Fiber 25% Glass fiber reinforced polyacetal for injection molding applications.Information provided by Polyram Ram On Ind. |
|||
Volume Resistivity | 1.00e+14 ohm-cm | 1.00e+14 ohm-cm | IEC 60093 |
DSM Akulon® S223-HPG5 Impact Modified Nylon 66-25% Glass Reinforced (European Grade) (Dry) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
Volume Resistivity | 1.00e+14 - 1.00e+15 ohm-cm @Temperature 23.0 °C |
1.00e+14 - 1.00e+15 ohm-cm @Temperature 73.4 °F |
ASTM D257 |
Daelim H&L Plavis G15 Aromatic Polyimide, 15% Graphite Filled, Machined Parts High abrasion resistance, very low friction coefficient property, suitable for being applied to spin component of spin apparatusInformation provided by Daelim H&L |
|||
Volume Resistivity | 1.00e+14 ohm-cm | 1.00e+14 ohm-cm | dry; IEC 60093 |
EMS-Grivory Grivory® TSG-35/4 H black 9836 PA666-GF35 Product description: Grilon TSG-35/4 H is a high heat stabilized, normal viscosity PA66 + PA6 injection molding grade with 35% glass fibers, modified for parts with high thermal demands. Grilon TSG-.. |
|||
Volume Resistivity | >= 1.00e+14 ohm-cm | >= 1.00e+14 ohm-cm | CEI 60093 |
Addiplast Addilene H 526 N30 Polypropylene Homopolymer Improved rigidity, high durabilityInformation provided by Addiplast. |
|||
Volume Resistivity | 1.00e+14 ohm-cm | 1.00e+14 ohm-cm | IEC 60093 |
BASF Ultramid® KR 4357 G6 BK 00564 30% Glass Filled PA6/6T (Dry) Description: 30% glass-fiber reinforced, impact-modified product for injection-molding; high toughness, strength and stiffness, low water absorption, high melting point (295°C [563°F]). The mechan.. |
|||
Volume Resistivity | 1.00e+14 ohm-cm | 1.00e+14 ohm-cm | |
3M EPS-300 Heat Shrink Tubing 3M Heat Shrink tubing EPS-300 is a 3:1 thin-wall, flexible tubing offering the advantages of integral, adhesive-lined construction. The tubing is made from flame-retardant, flexible polyolefin with .. |
|||
Volume Resistivity | 1.00e+14 ohm-cm | 1.00e+14 ohm-cm | Conditioned; CEI 60093 |
Addiplast Addinyl PMD 20104 Nylon 66 High molding rateInformation provided by Addiplast. |
|||
Volume Resistivity | 1.00e+14 ohm-cm | 1.00e+14 ohm-cm | ASTM D257 |
Techmer ES HiFill FR® PA6/6 GF50 FR-N BK 50% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 50% Filler by WeightFeatures: Flame Retardant and Halogen FreeAppearance: BlackInformation provided by TP Composites, Inc... |