Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 1.0 - 10 ohm-cm | 1.0 - 10 ohm-cm | ASTM D257 |
PolyOne Stat-Tech™ PK-30NCF/10T PEEK - 30% Nickel Coated Carbon Fiber - 10% PTFE
(discontinued **) Data provided by PolyOne. |
|||
Volume Resistivity | 1.0 - 10 ohm-cm | 1.0 - 10 ohm-cm | ASTM D257 |
PolyOne Stat-Tech™ AS-15NCF/000 ABS - 15% Nickel Coated Carbon Fiber
(discontinued **) Data provided by PolyOne. |
|||
Volume Resistivity | 1.0 ohm-cm | 1.0 ohm-cm | ASTM D257 |
Techmer ES Electrablend® PA6/6 05012 Availability: North AmericaForms: PelletsFiller/Reinforcement: Unspecified Filler/Reinfor.Features: ConductiveInformation provided by TP Composites, Inc. |
|||
Volume Resistivity | 1.0 - 1000 ohm-cm | 1.0 - 1000 ohm-cm | ASTM D257 |
Techmer ES Electrablend® PC 04003 FR BK Stainless Steel Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Stainless Steel FiberFeatures: Electromagnetic Shielding (EMI) and Flame RetardantAppearance: BlackTPCI# 9691124Information provided by.. |
|||
Volume Resistivity | 1.0 - 1000 ohm-cm | 1.0 - 1000 ohm-cm | ASTM D257 |
Techmer ES Electrablend® PC 04005 FR BK Stainless Steel Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Stainless Steel FiberFeatures: Electromagnetic Shielding (EMI) and Flame RetardantAppearance: BlackTPCI# 9691124Information provided by.. |
|||
Volume Resistivity | 1.0 - 1000 ohm-cm | 1.0 - 1000 ohm-cm | ASTM D257 |
Techmer ES Electrablend® PC 04006 FR BK Stainless Steel Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Stainless Steel FiberFeatures: Electromagnetic Shielding (EMI) and Flame RetardantAppearance: BlackInformation provided by TP Composite.. |
|||
Volume Resistivity | 1.0 - 1000 ohm-cm | 1.0 - 1000 ohm-cm | ASTM D257 |
Techmer ES Electrablend® PEI 04001 MB Stainless Steel Fiber Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Stainless Steel FiberFeatures: Electromagnetic Shielding (EMI)Information provided by TP Composites, Inc. |
|||
Volume Resistivity | 1.0 - 10 ohm-cm | 1.0 - 10 ohm-cm | ASTM D648 |
Techmer ES Electrafil® J-1200/CF/20 NAT ABS |
|||
Volume Resistivity | 1.0 - 10 ohm-cm | 1.0 - 10 ohm-cm | ASTM D648 |
Techmer ES Electrafil® J-80/CF/20 NAT Acetal (POM) Copolymer |
|||
Volume Resistivity | 1.0 ohm-cm | 1.0 ohm-cm | IEC 60093 |
SABIC Innovative Plastics LNP STAT-KON Valox_VCF2020 PET LNP* Stat-kon* Valox_VCF2020 compound is a 20% carbon fiber reinforced PET. Conductive applications. |
|||
Volume Resistivity | 1.0 - 100 ohm-cm | 1.0 - 100 ohm-cm | ASTM D257 |
Techmer ES Electrablend® ABS 03011 BK MB Availability: North AmericaForms: PelletsFiller/Reinforcement: Unspecified Filler/Reinfor.Features: Conductive, Electromagnetic Shielding (EMI) and Radio Frequency Shielding (RFI)Appearance: BlackIn.. |
|||
Volume Resistivity | 1.0 - 10 ohm-cm | 1.0 - 10 ohm-cm | ASTM D257 |
Techmer ES Electrablend® ABS SS15 BK MB 15% Stainless Steel Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Stainless Steel Fiber, 15% Filler by WeightFeatures: Electromagnetic Shielding (EMI)Appearance: BlackInformation provided by TP Composi.. |
|||
Volume Resistivity | 1.0 - 10 ohm-cm | 1.0 - 10 ohm-cm | ASTM D257 |
Techmer ES Electrablend® PA6 04001 BL Glass/Stainless Steel Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass/Stainless Steel FiberAdditive: LubricatedFeatures: Electromagnetic Shielding (EMI), Lubricated and Radio Frequency Shielding (RFI.. |
|||
Volume Resistivity | 1.0 - 10 ohm-cm | 1.0 - 10 ohm-cm | ASTM D257 |
Techmer ES Electrablend® PA6 04001 FR MB Glass/Stainless Steel Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass/Stainless Steel FiberAdditive: LubricatedFeatures: Electromagnetic Shielding (EMI), Lubricated, Flame Retardant and Radio Frequen.. |
|||
Volume Resistivity | 1.0 ohm-cm | 1.0 ohm-cm | 40% Carbon Black in HDPE |
TIMCAL ENSACO™ 250G Conductive Carbon Black ENSACO™ & SUPER P™ conductive carbon blacks are carbon blacks with a high to very high void volume allowing the retention of a carbon network at low to very low filler content. The void volume can.. |